Aluminum 357.0 sand cast T6 General Information
| Property | Value |
|---|---|
| Designation | 357.0 (Aluminum Association) |
| Condition | T6 (Solution heat-treated and artificially aged) |
| UNS Number | A03570 |
| Aluminum 357.0 sand cast T6 General Information |
Typical Uses for Aluminum 357.0 sand cast T6:
| Typical Use | Description |
|---|---|
| Space Frames | Used in lightweight structures for automotive applications |
| Wheels | Used in automotive wheels for strength and weight reduction |
| Axle and Differential Housings | Applied in critical automotive components requiring high strength |
| Pump and Meter | Utilized in automotive and industrial pumps and meters for fluid transfer |
| Intake Manifolds | Used in engine components for distributing air/fuel mixture |
| Electronic Cases | Used in protective casings for electronics requiring thermal conductivity |
| Fuel Pumps | Applied in automotive fuel pumps for strength and corrosion resistance |
| Typical Uses for Aluminum 357.0 sand cast T6 |
MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Plaster Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated and CNC Machined Products Manufacturer in Turkey