Aluminum 357.0 sand cast T6 Mechanical Properties
| Property | Value |
|---|---|
| Young’s modulus | 70.6 – 73.4 GPa |
| Specific stiffness | 26 – 27.1 MN.m/kg |
| Yield strength (elastic limit) | 281 – 311 MPa |
| Tensile strength | 345 – 380 MPa |
| Specific strength | 104 – 115 kN.m/kg |
| Elongation | 2 – 2.4 % strain |
| Compressive strength | 109 – 121 MPa |
| Flexural modulus | 70.6 – 73.4 GPa |
| Flexural strength (modulus of rupture) | 296 – 326 MPa |
| Shear modulus | 26.4 – 27.8 GPa |
| Bulk modulus | 66.1 – 75.5 GPa |
| Poisson’s ratio | 0.322 – 0.338 |
| Shape factor | 23 |
| Hardness – Vickers | 100 – 110 HV |
| Elastic stored energy (springs) | 550 – 670 kJ/m³ |
| Fatigue strength at 10^7 cycles | 55.8 – 68.2 MPa |
| Fatigue strength model (stress range) | 53.9 – 70.6 MPa |
| Aluminum 357.0 sand cast T6 Mechanical Properties |
MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Plaster Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated and CNC Machined Products Manufacturer in Turkey