Aluminum, 357.0, sand cast, T6 | Mechanical Properties

Aluminum 357.0 sand cast T6 Mechanical Properties Property Value Young’s modulus 70.6 – 73.4 GPa Specific stiffness 26 – 27.1 MN.m/kg Yield strength (elastic limit) 281 – 311 MPa Tensile strength 345 – 380 MPa Specific strength 104 – 115 kN.m/kg Elongation 2 – 2.4 % strain Compressive strength 109 – 121 MPa Flexural modulus … Continue reading Aluminum, 357.0, sand cast, T6 | Mechanical Properties