Aluminum 357.0 sand cast T6 Equivalent Grades
| Region | Standard |
| Australia | AA603 to AS 1874, AC603 to AS 1874 |
| Europe | EN AB-42200 to CEN EN 1676, EN AC-42200 to CEN EN 1706 |
| France | A-S7G06 to NF A50-702 |
| South Africa | Al-Si7Mg0.6 to SABS 991 |
| Sweden | 4245 to MNC 41E |
| USA | 357, 357 to ASTM B108, 357.1, 357.1 to ASTM B179 |
| 357.1 to QQ A-371F, A03570 to SAE J452, A357.2 to ASTM B179 | |
| B356.2, B357.0, B357.2, C356.2 | |
| UNS A03570, UNS A03571, UNS A23562, UNS A23570, UNS A23572 | |
| UNS A33562, UNS A53570, UNS A53571 | |
| Aluminum 357.0 sand cast T6 Equivalent Grades |
Aluminum 357.0 sand cast T6 Tradenames
| Tradenames |
|---|
| ALUMINUM 357 |
| ALUMINUM X357 |
| CALYPSO 67 N1 |
| TA-356 |
| TECHNI-CAST A-356 |
| Aluminum 357.0 sand cast T6 Tradenames |
MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Plaster Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated and CNC Machined Products Manufacturer in Turkey