Mechanical Properties for Aluminum 336.0
| Property | Value Range | Units |
|---|---|---|
| Young’s Modulus | 72.5 – 75.5 | GPa |
| Specific Stiffness | 26.7 – 27.9 | MN·m/kg |
| Yield Strength (Elastic Limit) | 183 – 203 | MPa |
| Tensile Strength | 236 – 260 | MPa |
| Specific Strength | 67.4 – 74.9 | kN·m/kg |
| Elongation | 1 – 2 | % strain |
| Compressive Strength | 183 – 203 | MPa |
| Flexural Modulus | 73.5 – 76.5 | GPa |
| Flexural Strength (Modulus of Rupture) | 183 – 203 | MPa |
| Shear Modulus | 27.5 – 28.9 | GPa |
| Bulk Modulus | 68.8 – 78.7 | GPa |
| Poisson’s Ratio | 0.322 – 0.338 | Dimensionless |
| Shape Factor | 32 | Dimensionless |
| Hardness (Vickers) | 111 – 123 | HV |
| Elastic Stored Energy (Springs) | 227 – 278 | kJ/m³ |
| Fatigue Strength at 10⁷ Cycles | 83.7 – 102 | MPa |
| Fatigue Strength Model (Stress Range) | 80.8 – 106 | MPa |
| Aluminum, 336.0, permanent mold cast, T551 | Mechanical Properties | Aluminum UNS A03360 Mechanical Properties |
MODULUS METAL | ALUMINUM CASTING FOUNDRY IN TURKEY
Aluminium Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Plaster Casting in Turkey, Heat Treated and CNC Machined Products Manufacturer in Turkey