Aluminum, 336.0, permanent mold cast, T551 | Composition

Composition Overview for Aluminum 336.0 Category Details Compositional Summary Al79-86 / Si11-13 / Ni2-3 / Cu0.5-1.5 / Mg0.7-1.3 (impurities: Fe<1.2, Mn<0.35, Zn<0.35, Ti<0.25, Other<0.05) Material Family Metal (non-ferrous) Base Material Al (Aluminum) Aluminum, 336.0, permanent mold cast, T551 | Composition Overview Aluminum UNS A03360 Composition Overview Composition Details Element Composition Range (%) Al (aluminum) 79 … Continue reading Aluminum, 336.0, permanent mold cast, T551 | Composition