Aluminum, 336.0, permanent mold cast, T551 | General Information

General Information for Aluminum 336.0

AttributeValue
Designation336.0 (Aluminum Association)
ConditionT551 (Cooled from an elevated-temperature shaping process and artificially aged)
UNS NumberA03360
Aluminum, 336.0, permanent mold cast, T551 | General InformationAluminum UNS A03360 General Information

Typical Uses for Aluminum 336.0

ApplicationDetails
High-temperature alloyPistons, cylinder heads, gear housings, other engine parts