Aluminum, 336.0, permanent mold cast, T551 | General Information
General Information for Aluminum 336.0 Attribute Value Designation 336.0 (Aluminum Association) Condition T551 (Cooled from an elevated-temperature shaping process and artificially aged) UNS Number A03360 Aluminum, 336.0, permanent mold cast, T551 | General Information Aluminum UNS A03360 General Information Typical Uses for Aluminum 336.0 Application Details High-temperature alloy Pistons, cylinder heads, gear housings, other engine … Continue reading Aluminum, 336.0, permanent mold cast, T551 | General Information