Aluminum, 336.0, permanent mold cast, T551 | Composition

Composition Overview for Aluminum 336.0

CategoryDetails
Compositional SummaryAl79-86 / Si11-13 / Ni2-3 / Cu0.5-1.5 / Mg0.7-1.3 (impurities: Fe<1.2, Mn<0.35, Zn<0.35, Ti<0.25, Other<0.05)
Material FamilyMetal (non-ferrous)
Base MaterialAl (Aluminum)
Aluminum, 336.0, permanent mold cast, T551 | Composition Overview Aluminum UNS A03360 Composition Overview

Composition Details

ElementComposition Range (%)
Al (aluminum)79 – 85.8
Si (silicon)11 – 13
Ni (nickel)2 – 3
Cu (copper)0.5 – 1.5
Mg (magnesium)0.7 – 1.3
Fe (iron)0 – 1.2
Mn (manganese)0 – 0.35
Zn (zinc)0 – 0.35
Ti (titanium)0 – 0.25
Other0 – 0.05
Aluminum, 336.0, permanent mold cast, T551 | CompositionDetailsAluminum UNS A03360 Composition Details

MODULUS METAL | ALUMINUM CASTING FOUNDRY IN TURKEY
Aluminium Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Plaster Casting in Turkey, Heat Treated and CNC Machined Products Manufacturer in Turkey