Aluminum, 336.0, permanent mold cast, T551 | Mechanical Properties

Mechanical Properties for Aluminum 336.0 Property Value Range Units Young’s Modulus 72.5 – 75.5 GPa Specific Stiffness 26.7 – 27.9 MN·m/kg Yield Strength (Elastic Limit) 183 – 203 MPa Tensile Strength 236 – 260 MPa Specific Strength 67.4 – 74.9 kN·m/kg Elongation 1 – 2 % strain Compressive Strength 183 – 203 MPa Flexural Modulus … Continue reading Aluminum, 336.0, permanent mold cast, T551 | Mechanical Properties