Mechanical properties

PropertyValue (Min)Value (Max)Units
Young’s modulus68.671.4GPa
Specific stiffness24.525.6MN.m/kg
Yield strength (elastic limit)170188MPa
Tensile strength276304MPa
Specific strength60.867.3kN.m/kg
Elongation56% strain
Compressive strength171189MPa
Flexural modulus68.671.4GPa
Flexural strength (modulus of rupture)179197MPa
Shear modulus25.627GPa
Bulk modulus64.273.5GPa
Poisson’s ratio0.3220.338–
Shape factor33––
Hardness – Vickers100110HV
Elastic stored energy (springs)207252kJ/m³
Fatigue strength at 10^7 cycles6377MPa
Fatigue strength model (stress range)60.979.7MPa
Aluminum 296.0, permanent mold cast, T6 | Mechanical properties
(UNS A020960 Mechanical properties)

MODULUS METAL | ALUMINUM CASTING FOUNDRY IN TURKEY
Aluminium Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, Investment Casting in Turkey, Plaster Casting in Turkey, Heat Treated and CNC Machined Products Manufacturer in Turkey