Composition Overview
Compositional Summary | Al89-94 / Cu4-5 / Si2-3 (Impurities: Fe<1.2, Zn<0.5, Mn<0.35, Ni<0.35, Ti<0.25, Mg<0.05, Other<0.35) |
Material Family | Metal (non-ferrous) |
Base Material | Al (Aluminum) |
Aluminum 296.0 Composition, UNS A020960 Composition |
Composition Detail
Element | Symbol | Minimum (%) | Maximum (%) |
---|---|---|---|
Aluminum | Al | 89 | 94 |
Copper | Cu | 4 | 5 |
Iron | Fe | 0 | 1.2 |
Magnesium | Mg | 0 | 0.05 |
Manganese | Mn | 0 | 0.35 |
Nickel | Ni | 0 | 0.35 |
Silicon | Si | 2 | 3 |
Titanium | Ti | 0 | 0.25 |
Zinc | Zn | 0 | 0.5 |
Other Elements | – | 0 | 0.35 |
Aluminum 296.0 Composition, UNS A020960 Composition |
Aluminum, 296.0, permanent mold cast, T6 | General Information
Aluminum 296.0, permanent mold cast, T6 | Composition
Aluminum 296.0, permanent mold cast, T6 | Mechanical properties
Aluminum, 296.0, permanent mold cast, T6 Equivalent Grades
MODULUS METAL | ALUMINUM CASTING FOUNDRY IN TURKEY
Aluminium Sand Casting, Permanent Mold Casting, Gravity Die Casting, Pressure Die Casting, Investment Casting, Plaster Casting, Heat Treated and CNC Machined Products Manufacturer in Turkey