| Material | Specification/Standard |
|---|---|
| Aluminum, 296.0, Permanent Mold Cast, T6 | |
| USA Standards with Similar Compositions | |
| 208 | ASTM B108, ASTM B26/B26M, ASTM B618 |
| 208.1 | ASTM B179 |
| 296 | ASTM B108 |
| 296.1 | ASTM B179 |
| 296.2 | ASTM B179 |
| A02080 | SAE J452 |
| A02960 | SAE J452 |
| B295.1 | QQ A-371F |
| B295.2 | QQ A-371F |
| UNS A02080 | |
| UNS A02081 | |
| UNS A02960 | |
| UNS A02961 | |
| UNS A02962 | |
| Aluminum, 296.0, permanent mold cast, T6 Equivalent Grades (UNS A020960 Equivalent Grades) |
| Tradenames: Aluminum, 296.0, permanent mold cast, T6 (UNS A020960) |
|---|
| ALCOA B 105 |
| ALLCAST 53 |
| USCO C-2 |
| UNS A020960 Tradenames |
Aluminum, 296.0, permanent mold cast, T6 | General Information
Aluminum 296.0, permanent mold cast, T6 | Composition
Aluminum 296.0, permanent mold cast, T6 | Mechanical properties
Aluminum, 296.0, permanent mold cast, T6 Equivalent Grades
MODULUS METAL | ALUMINUM CASTING FOUNDRY IN TURKEY
Aluminium Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, Investment Casting in Turkey, Plaster Casting in Turkey, Heat Treated and CNC Machined Products Manufacturer in Turkey