General Information
| Designation | 296.0 (Aluminum Association) |
| Condition | T6 (Solution heat-treated and artificially aged) |
| UNS Number | A020960, ~A02950 |
| Typical Uses | High tensile properties and good machinability: aircraft fittings, wheels, railroad car seat frames, compressor rods, pump bodies |
| Aluminum, 296.0, permanent mold cast, T6 General Information |
Aluminum, 296.0, permanent mold cast, T6 | General Information
Aluminum 296.0, permanent mold cast, T6 | Composition
Aluminum 296.0, permanent mold cast, T6 | Mechanical properties
Aluminum, 296.0, permanent mold cast, T6 Equivalent Grades