AISI 1040, As Rolled, Mechanical properties

Young’s modulus208–216GPa
Specific stiffness26.5–27.5MN.m/kg
Yield strength (elastic limit)375–460MPa
Tensile strength565–690MPa
Specific strength47.8–58.6kN.m/kg
Elongation20–30% strain
Compressive strength375–460MPa
Flexural modulus208–216GPa
Flexural strength (modulus of rupture)375–460MPa
Shear modulus80–85GPa
Bulk modulus161–176GPa
Poisson’s ratio0.285–0.295 
Shape factor54   
Hardness – Vickers188–228HV
Elastic stored energy (springs)335–495kJ/m^3
Fatigue strength at 10^7 cycles287–331MPa
Fatigue strength model (stress range) Parameters: Stress Ratio = -1, Number of Cycles = 1e7cycles251–379MPa
AISI 1040, As Rolled, Mechanical properties

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey