AISI 1040, Normalized, Mechanical properties

Young’s modulus208–216GPa
Specific stiffness26.5–27.5MN.m/kg
Yield strength (elastic limit)335–415MPa
Tensile strength530–650MPa
Specific strength42.7–52.9kN.m/kg
Elongation22–34% strain
Compressive strength335–415MPa
Flexural modulus208–216GPa
Flexural strength (modulus of rupture)335–415MPa
Shear modulus80–85GPa
Bulk modulus161–176GPa
Poisson’s ratio0.285–0.295 
Shape factor57   
Hardness – Vickers160–195HV
Elastic stored energy (springs)267–402kJ/m^3
Fatigue strength at 10^7 cycles274–317MPa
Fatigue strength model (stress range)
Parameters: Stress Ratio = -1, Number of Cycles = 1e7cycles
238–365MPa

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey