AISI 1040 Carbon Steel Chemical Composition

AISI 1040 Composition overview

Compositional summary
Fe99 / Mn0.6-0.9 / C0.37-0.44 (impurities: S<0.05, P<0.04)
Material familyMetal (ferrous)
Base materialFe (Iron)

AISI 1040 Composition Detail

C (carbon)0.37–0.44%
Fe (iron)98.6–99%
Mn (manganese)0.6–0.9%
P (phosphorus)0–0.04%
S (sulfur)0–0.05%

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey