AISI 1040, Normalized, Mechanical properties Young’s modulus 208 – 216 GPa Specific stiffness 26.5 – 27.5 MN.m/kg Yield strength (elastic limit) 335 – 415 MPa Tensile strength 530 – 650 MPa Specific strength 42.7 – 52.9 kN.m/kg Elongation 22 – 34 % strain Compressive strength 335 – 415 MPa Flexural modulus 208 – 216 GPa … Continue reading AISI 1040 Carbon Steel Normalized Mechanical Properties