Home » PA (Polyamide / Nylon) » PPA (Polyphthalamide) » PPA Glass Filled Grades » PPA 45% Glass Fiber Flame Retarded Material Data Sheet
PPA 45% Glass Fiber Flame Retarded (Polyphthalamide) Material Data Sheet
PPA 45% Glass Fiber Flame Retarded Overview
PPA 45% glass fiber flame retarded is a grade of polyphthalamide (PPA), designated Polyphthalamide (45% glass fiber, V-0). This PPA 45% glass fiber flame retarded material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PPA parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PPA parts in-house and inspects them before shipment.
PPA 45% Glass Fiber Flame Retarded Designation
Polyphthalamide (45% glass fiber, V-0) Tradenames Amodel
PPA 45% Glass Fiber Flame Retarded Typical uses
Industrial and chemical processing equipment, bearings, gears, electrical connectors, packaging, under bonnet automobile applications
PPA 45% Glass Fiber Flame Retarded Composition detail
Polymer 40 – 50 % Flame retardant 5 – 15 % Glass (fiber) 45 %
PPA 45% Glass Fiber Flame Retarded Physical properties
PPA 45% Glass Fiber Flame Retarded Mechanical properties
Young’s modulus 16 – 20 GPa Specific stiffness 8.84 – 11.1 MN.m/kg Yield strength (elastic limit) 138 – 172 MPa Tensile strength 140 – 171 MPa Specific strength 76.2 – 95.1 kN.m/kg Elongation 1.23 – 1.77 % strain Elongation at yield 1.04 – 1.97 % strain Compressive modulus 17.1 – 18.9 GPa Compressive strength 177 – 195 MPa Flexural modulus 13.8 – 16.6 GPa Flexural strength (modulus of rupture) 234 – 286 MPa Shear modulus 6.56 – 6.89 GPa Shear strength 83.7 – 102 MPa Bulk modulus 17.6 – 19.4 GPa Poisson’s ratio 0.325 – 0.338 Shape factor 9.08 Hardness – Vickers 44 – 49 HV Hardness – Rockwell M 179 – 197 Hardness – Rockwell R 179 – 197 Hardness – Shore D 97 – 101 Elastic stored energy (springs) 526 – 837 kJ/m3 Fatigue strength at 10^7 cycles 58.9 – 65.1 MPa
PPA 45% Glass Fiber Flame Retarded Impact & fracture properties
Fracture toughness 5.48 – 6.06 MPa.m0.5 Toughness (G) 1.6 – 2.15 kJ/m2 Impact strength, notched 23 °C 4.08 – 7.92 kJ/m2 Impact strength, notched -30 °C 3.84 – 8.36 kJ/m2 Impact strength, unnotched 23 °C 22.7 – 33.3 kJ/m2 Impact strength, unnotched -30 °C 22 – 33 kJ/m2
PPA 45% Glass Fiber Flame Retarded Thermal properties
Melting point 299 – 322 °C Glass temperature 119 – 135 °C Heat deflection temperature 0.45MPa 274 – 329 °C Heat deflection temperature 1.8MPa 249 – 302 °C Maximum service temperature 210 – 229 °C Minimum service temperature -49 – -29 °C Thermal conductivity 0.651 – 0.677 W/m.°C Specific heat capacity 1160 – 1210 J/kg.°C Thermal expansion coefficient 15 – 55 µstrain/°C Thermal shock resistance 155 – 579 °C Thermal distortion resistance 0.0121 – 0.0442 MW/m
PPA 45% Glass Fiber Flame Retarded Electrical properties
Electrical resistivity 2e20 – 5e21 µohm.cm Electrical conductivity 3.45e-20 – 8.62e-19 %IACS Dielectric constant (relative permittivity) 3.53 – 4.98 Dissipation factor (dielectric loss tangent) 0.0102 – 0.027 Dielectric strength (dielectric breakdown) 22.2 – 37.8 MV/m Comparative tracking index 600 V
PPA 45% Glass Fiber Flame Retarded Magnetic properties
Magnetic type Non-magnetic
PPA 45% Glass Fiber Flame Retarded Optical, aesthetic and acoustic properties
Transparency Opaque Acoustic velocity 2970 – 3330 m/s Mechanical loss coefficient (tan delta) 0.00645 – 0.00713
PPA 45% Glass Fiber Flame Retarded Absorption & permeability
Water absorption @ 24 hrs 0.23 – 0.37 % Water absorption @ sat 4.6 – 6 % Humidity absorption @ sat 0.85 – 1.2 %
PPA 45% Glass Fiber Flame Retarded Processing properties
Polymer injection molding Acceptable Polymer extrusion Unsuitable Polymer thermoforming Limited use Linear mold shrinkage 0.182 – 0.22 % Melt temperature 263 – 338 °C Molding pressure range 34.4 – 103 MPa
PPA 45% Glass Fiber Flame Retarded Durability
Water (fresh) Excellent Water (salt) Excellent Weak acids Excellent Strong acids Limited use Weak alkalis Excellent Strong alkalis Limited use Organic solvents Limited use Oxidation at 500C Unacceptable UV radiation (sunlight) Fair Flammability Self-extinguishing