PARA 30% Glass Fiber Material Data Sheet

PARA 30% Glass Fiber (Polyarylamide) Material Data Sheet

PARA 30% Glass Fiber Overview

PARA 30% glass fiber is a grade of polyarylamide (PARA), designated Polyarylamide (30% glass fiber). This PARA 30% glass fiber material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PARA parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PARA parts in-house and inspects them before shipment.

PARA 30% Glass Fiber Designation

Polyarylamide (30% glass fiber)
TradenamesGlamide, Ixef, Reny

PARA 30% Glass Fiber Typical uses

Automotive, furniture, small appliances, lawn mowers, power tools, electrical contactors and switches, electrical motor components, cell phones, faucet components.

PARA 30% Glass Fiber Composition detail

Polymer70  %
Glass (fiber)30  %

PARA 30% Glass Fiber Physical properties

Density1.42–1.45g/cm3

PARA 30% Glass Fiber Mechanical properties

Young’s modulus9.06–11.3GPa
Specific stiffness6.31–7.88MN.m/kg
Yield strength (elastic limit)140–174MPa
Tensile strength150–183MPa
Specific strength97.5–121kN.m/kg
Elongation1.94–2.79% strain
Elongation at yield1.63–3.1% strain
Compressive modulus9.67–10.7GPa
Compressive strength190–210MPa
Flexural modulus9.26–11.1GPa
Flexural strength (modulus of rupture)222–272MPa
Shear modulus3.68–3.87GPa
Shear strength90–110MPa
Bulk modulus10.6–11.7GPa
Poisson’s ratio0.346–0.348 
Shape factor6.17
Hardness – Vickers45–50HV
Hardness – Rockwell M184–204 
Hardness – Rockwell R184–204 
Hardness – Shore D98–102 
Elastic stored energy (springs)957–1510kJ/m3
Fatigue strength at 10^7 cycles63.3–70MPa

PARA 30% Glass Fiber Impact & fracture properties

Fracture toughness4.89–5.4MPa.m0.5
Toughness (G)2.26–3.01kJ/m2
Impact strength, notched 23 °C5.21–10.1kJ/m2
Impact strength, unnotched 23 °C18.7–27.5kJ/m2

PARA 30% Glass Fiber Thermal properties

Melting point267–292°C
Glass temperature78–92.2°C
Heat deflection temperature 0.45MPa247–268°C
Heat deflection temperature 1.8MPa220–240°C
Vicat softening point77–90°C
Maximum service temperature186–207°C
Thermal conductivity0.485–0.497W/m.°C
Specific heat capacity1390–1410J/kg.°C
Thermal expansion coefficient17.6–18.5µstrain/°C
Thermal shock resistance735–999°C
Thermal distortion resistance0.0265–0.0281MW/m

PARA 30% Glass Fiber Electrical properties

Electrical resistivity2e20–5e21µohm.cm
Electrical conductivity3.45e-20–8.62e-19%IACS
Dielectric constant (relative permittivity)3.45–4.86 
Dissipation factor (dielectric loss tangent)0.012–0.0318 
Dielectric strength (dielectric breakdown)22–37.4MV/m
Comparative tracking index400–450V

PARA 30% Glass Fiber Magnetic properties

Magnetic typeNon-magnetic

PARA 30% Glass Fiber Optical, aesthetic and acoustic properties

TransparencyOpaque
Acoustic velocity2510–2810m/s
Mechanical loss coefficient (tan delta)0.00788–0.00871 

PARA 30% Glass Fiber Absorption & permeability

Water absorption @ 24 hrs0.15–0.25%
Water absorption @ sat3.7–4.9%
Humidity absorption @ sat1.6–2.2%

PARA 30% Glass Fiber Processing properties

Polymer injection moldingLimited use
Polymer extrusionAcceptable
Polymer thermoformingLimited use
Linear mold shrinkage0.1 – 0.4 %
Melt temperature267 – 292 °C
Mold temperature116 – 144 °C
Molding pressure range30 – 150 MPa

PARA 30% Glass Fiber Durability

Water (fresh)Excellent
Water (salt)Acceptable
Weak acidsUnacceptable
Strong acidsUnacceptable
Weak alkalisAcceptable
Strong alkalisLimited use
Organic solventsLimited use
Oils and fuelsAcceptable
Oxidation at 500CUnacceptable
UV radiation (sunlight)Good
FlammabilitySlow-burning