PA6 Cast Plasticized (Polyamide 6) Material Data Sheet
PA6 Cast Plasticized Overview
PA6 cast plasticized is a grade of polyamide 6 (PA6, nylon 6), designated Polyamide (Nylon) (Type 6, Cast, Plasticized). This PA6 cast plasticized material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA6 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined cast PA6 parts in-house and inspects them before shipment.
PA6 Cast Plasticized Designation
Polyamide (Nylon) (Type 6, Cast, Plasticized)
Tradenames
Ashlene, Domamid, Grilon, Radici
PA6 Cast Plasticized Typical uses
Gears, cams, rollers, bearings, nuts and bolts, power tool housing, electrical connectors, combs, coil formers, fuel tanks for cars, kitchen utensils.
PA6 Cast Plasticized Composition detail
Polymer
77
–
83
%
Plasticizer/oil
17
–
23
%
PA6 Cast Plasticized Physical properties
Density
1.09
–
1.12
g/cm3
PA6 Cast Plasticized Mechanical properties
Young’s modulus
1.2
–
1.5
GPa
Specific stiffness
1.09
–
1.36
MN.m/kg
Yield strength (elastic limit)
35.6
–
44.4
MPa
Tensile strength
45
–
55
MPa
Specific strength
32.2
–
40.2
kN.m/kg
Elongation
20.5
–
29.5
% strain
Elongation at yield
6.77
–
12.9
% strain
Compressive modulus
1.28
–
1.42
GPa
Compressive strength
57
–
63
MPa
Flexural modulus
1.23
–
1.47
GPa
Flexural strength (modulus of rupture)
57.4
–
70.1
MPa
Shear modulus
0.469
–
0.493
GPa
Shear strength
27
–
33
MPa
Bulk modulus
2.2
–
2.44
GPa
Poisson’s ratio
0.387
–
0.403
Shape factor
4.3
Hardness – Vickers
11
–
13
HV
Hardness – Rockwell M
100
–
110
Hardness – Rockwell R
100
–
110
Hardness – Shore D
77
–
80
Elastic stored energy (springs)
467
–
743
kJ/m3
Fatigue strength at 10^7 cycles
19
–
21
MPa
PA6 Cast Plasticized Impact & fracture properties
Fracture toughness
3.25
–
3.59
MPa.m0.5
Toughness (G)
7.52
–
10.1
kJ/m2
Impact strength, notched 23 °C
8.06
–
15.6
kJ/m2
PA6 Cast Plasticized Thermal properties
Melting point
227
–
238
°C
Glass temperature
44
–
56
°C
Heat deflection temperature 0.45MPa
204
–
221
°C
Heat deflection temperature 1.8MPa
166
–
204
°C
Maximum service temperature
52
–
67
°C
Minimum service temperature
-64
–
-54
°C
Thermal conductivity
0.273
–
0.284
W/m.°C
Specific heat capacity
1580
–
1640
J/kg.°C
Thermal expansion coefficient
79.4
–
82.6
µstrain/°C
Thermal shock resistance
313
–
427
°C
Thermal distortion resistance
0.00334
–
0.00353
MW/m
PA6 Cast Plasticized Electrical properties
Electrical resistivity
2e17
–
5e18
µohm.cm
Electrical conductivity
3.45e-17
–
8.62e-16
%IACS
Dielectric constant (relative permittivity)
5.4
–
7.61
Dissipation factor (dielectric loss tangent)
0.0825
–
0.218
Dielectric strength (dielectric breakdown)
10.4
–
17.6
MV/m
Comparative tracking index
600
V
PA6 Cast Plasticized Magnetic properties
Magnetic type
Non-magnetic
PA6 Cast Plasticized Optical, aesthetic and acoustic properties