PA6 Cast Oil-Filled (Polyamide 6) Material Data Sheet
PA6 Cast Oil-Filled Overview
PA6 cast oil-filled is a grade of polyamide 6 (PA6, nylon 6), designated Polyamide (Nylon) (Type 6, Cast, Oil-filled). This PA6 cast oil-filled material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA6 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined cast PA6 parts in-house and inspects them before shipment.
PA6 Cast Oil-Filled Designation
Polyamide (Nylon) (Type 6, Cast, Oil-filled)
Tradenames
Ashlene, Domamid, Grilon, Radici
PA6 Cast Oil-Filled Typical uses
Gears, cams, rollers, bearings, nuts and bolts, power tool housing, electrical connectors, combs, coil formers, fuel tanks for cars, kitchen utensils.
PA6 Cast Oil-Filled Composition detail
Polymer
67
–
73
%
Plasticizer/oil
27
–
33
%
PA6 Cast Oil-Filled Physical properties
Density
1.12
–
1.15
g/cm3
PA6 Cast Oil-Filled Mechanical properties
Young’s modulus
1.29
–
1.61
GPa
Specific stiffness
1.14
–
1.42
MN.m/kg
Yield strength (elastic limit)
40.1
–
50
MPa
Tensile strength
50.6
–
61.9
MPa
Specific strength
35.3
–
44.1
kN.m/kg
Elongation
41
–
59
% strain
Elongation at yield
5.58
–
10.6
% strain
Compressive modulus
1.38
–
1.52
GPa
Compressive strength
64.1
–
70.9
MPa
Flexural modulus
1.32
–
1.58
GPa
Flexural strength (modulus of rupture)
66.2
–
80.9
MPa
Shear modulus
0.52
–
0.546
GPa
Shear strength
30.4
–
37.1
MPa
Bulk modulus
1.64
–
1.81
GPa
Poisson’s ratio
0.34
–
0.36
Shape factor
4.3
Hardness – Vickers
13
–
14
HV
Hardness – Rockwell M
107
–
118
Hardness – Rockwell R
107
–
118
Hardness – Shore D
79
–
83
Elastic stored energy (springs)
552
–
877
kJ/m3
Fatigue strength at 10^7 cycles
21.4
–
23.6
MPa
PA6 Cast Oil-Filled Impact & fracture properties
Fracture toughness
3.3
–
3.64
MPa.m0.5
Toughness (G)
7.22
–
9.62
kJ/m2
Impact strength, notched 23 °C
10.7
–
20.9
kJ/m2
PA6 Cast Oil-Filled Thermal properties
Melting point
227
–
238
°C
Glass temperature
44
–
56
°C
Heat deflection temperature 0.45MPa
204
–
221
°C
Heat deflection temperature 1.8MPa
166
–
204
°C
Maximum service temperature
52
–
67
°C
Minimum service temperature
-64
–
-54
°C
Thermal conductivity
0.261
–
0.271
W/m.°C
Specific heat capacity
1590
–
1650
J/kg.°C
Thermal expansion coefficient
61.7
–
64.3
µstrain/°C
Thermal shock resistance
423
–
575
°C
Thermal distortion resistance
0.00411
–
0.00434
MW/m
PA6 Cast Oil-Filled Electrical properties
Electrical resistivity
2e17
–
5e18
µohm.cm
Electrical conductivity
3.45e-17
–
8.62e-16
%IACS
Dielectric constant (relative permittivity)
5.4
–
7.61
Dissipation factor (dielectric loss tangent)
0.0825
–
0.218
Dielectric strength (dielectric breakdown)
10.4
–
17.6
MV/m
Comparative tracking index
600
V
PA6 Cast Oil-Filled Magnetic properties
Magnetic type
Non-magnetic
PA6 Cast Oil-Filled Optical, aesthetic and acoustic properties