PEKK (Polyetherketoneketone)

PEKK (Polyetherketoneketone)

PEKK Overview

PEKK (polyetherketoneketone) is a member of the PAEK family, which also includes PEEKK and the less common PEEKEK and PEEEK.

PEKK Strengths

PEKK has the highest melting temperature (391 °C (736 °F)) and the highest glass transition temperature (165 °C (330 °F)) of the commercial polyether ketones, and slightly better stiffness and tensile strength than PEEK.

PEKK Limitations

It costs more than PEEK and needs even higher mold temperatures than PEEK, which are already high.

Typical Uses of PEKK

Applications are similar to those of PEK, such as bearings, seals, gears and other high-temperature engineering components.

PEKK Compositional Summary

(-O-C6H4-CO-C6H4-CO-C6H4-)n
Material familyPlastic (thermoplastic, semi-crystalline)
Base materialPEKK (Polyetherketoneketone)

Effect of Composition on PEKK

PEKK can also be produced as a transparent amorphous grade, which has lower mechanical properties.

PEKK Notes

Amorphous grades are available.

PEKK Processing Properties

Forming

PEKK suits compression molding, injection molding and vacuum forming, while extrusion is difficult. It needs very high melt temperatures, and pre-drying is essential because of the high mold temperatures. Fine powder can coat metal parts up to about 2 mm thick by vortex sintering.

Machining

The material machines very easily. Carbide or diamond-tipped tools with water cooling are recommended, and the parts should be annealed before machining.

Joining

Solvent bonding is difficult, but a wide range of adhesives works well, and surface treatment such as laser treatment greatly improves bond strength. All welding methods except radio-frequency welding are suitable, although hot gas welding is difficult and the high melting point means welding needs a lot of energy. Laser welding works, the material can be welded to PEI, and welds to aluminum have had some success. Films can be heat sealed at high temperatures.

Surface Treatment

PEKK can be painted.

PEKK Grades

Unfilled PEKK

PEKK (unfilled, amorphous)

PEKK (unfilled, semi-crystalline)

Glass Filled PEKK

PEKK (30% glass fiber)

PEKK (40% glass fiber)

Carbon Filled PEKK

PEKK (30% carbon fiber)

PEKK (40% carbon fiber)