PEKK 40% Carbon Fiber Overview

PEKK 40% carbon fiber is a grade of polyetherketoneketone (PEKK), designated Polyetherketoneketone (40% carbon fiber). This PEKK 40% carbon fiber material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PEKK parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PEKK parts in-house and inspects them before shipment.

PEKK Designation

Polyetherketoneketone (40% carbon fiber)
TradenamesLuvocom, Oxpekk

PEKK 40% Carbon Fiber Composition detail

Polymer60  %
Carbon (fiber)40  %

PEKK Physical properties

Density1.44–1.46g/cm3

PEKK 40% Carbon Fiber Mechanical properties

Young’s modulus46.9–49.4GPa
Specific stiffness32.3–34.1MN.m/kg
Yield strength (elastic limit)247–272MPa
Tensile strength309–342MPa
Specific strength170–188kN.m/kg
Elongation1.2–1.4% strain
Elongation at yield1.2–1.4% strain
Compressive modulus46.9–49.4GPa
Flexural modulus30.2–31.8GPa
Flexural strength (modulus of rupture)437–459MPa
Shear modulus17–18GPa
Shear strength140–155MPa
Poisson’s ratio0.42–0.46 
Shape factor12.4
Hardness – Vickers73–80HV
Elastic stored energy (springs)633–769kJ/m3
Fatigue strength at 10^7 cycles124–137MPa

PEKK Impact & fracture properties

Impact strength, notched 23 °C9.35–9.64kJ/m2
Impact strength, unnotched 23 °C84.5–103kJ/m2

PEKK 40% Carbon Fiber Thermal properties

Melting point347–373°C
Glass temperature153–170°C
Heat deflection temperature 0.45MPa331–361°C
Heat deflection temperature 1.8MPa323–352°C
Vicat softening point331–361°C
Maximum service temperature233–287°C
Specific heat capacity1370–1390J/kg.°C
Thermal expansion coefficient5.38–9.62µstrain/°C
Thermal shock resistance558–1000°C

PEKK Electrical properties

Electrical resistivity9250000000000000–10800000000000000µohm.cm
Electrical conductivity1.6e-14–1.86e-14%IACS
Dielectric constant (relative permittivity)3.17–3.43 
Dissipation factor (dielectric loss tangent)0.0035–0.0045 
Dielectric strength (dielectric breakdown)23–25MV/m
Galvanic potential0.14–0.22V

PEKK Magnetic properties

Magnetic typeNon-magnetic

PEKK Optical, aesthetic and acoustic properties

TransparencyOpaque
Acoustic velocity5680–5840m/s

PEKK Absorption & permeability

Water absorption @ 24 hrs0.0317–0.0883%

PEKK Processing properties

Polymer injection moldingLimited use
Polymer extrusionLimited use
Polymer thermoformingUnsuitable
Linear mold shrinkage0.04 – 0.06 %

PEKK Durability

Water (fresh)Excellent
Water (salt)Excellent
Weak acidsExcellent
Strong acidsUnacceptable
Weak alkalisExcellent
Strong alkalisExcellent
Organic solventsExcellent
Oils and fuelsExcellent
Oxidation at 500CUnacceptable
UV radiation (sunlight)Excellent
FlammabilitySelf-extinguishing