PEKK 30% Glass Fiber Material Data Sheet

PEKK 30% Glass Fiber (Polyetherketoneketone) Material Data Sheet

PEKK 30% Glass Fiber Overview

PEKK 30% glass fiber is a grade of polyetherketoneketone (PEKK), designated Polyetherketoneketone (30% glass fiber). This PEKK 30% glass fiber material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PEKK parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PEKK parts in-house and inspects them before shipment.

PEKK Designation

Polyetherketoneketone (30% glass fiber)
TradenamesOxpekk

PEKK 30% Glass Fiber Composition detail

Polymer70  %
Glass (fiber)30  %

PEKK Physical properties

Density1.49–1.53g/cm3

PEKK 30% Glass Fiber Mechanical properties

Young’s modulus11.8–12.6GPa
Specific stiffness7.78–8.34MN.m/kg
Yield strength (elastic limit)144–153MPa
Tensile strength177–188MPa
Specific strength95.2–101kN.m/kg
Elongation1.75–1.98% strain
Elongation at yield1.8–2% strain
Compressive modulus11.8–12.6GPa
Compressive strength209–231MPa
Flexural modulus10.7–11.3GPa
Flexural strength (modulus of rupture)253–261MPa
Shear modulus4.4–4.7GPa
Shear strength80–89MPa
Poisson’s ratio0.41–0.45 
Shape factor7.18
Hardness – Vickers43–45HV
Hardness – Rockwell M98–108 
Elastic stored energy (springs)846–970kJ/m3
Fatigue strength at 10^7 cycles69.4–76.7MPa

PEKK Impact & fracture properties

Impact strength, notched 23 °C8.62–9.74kJ/m2
Impact strength, unnotched 23 °C72.1–88.1kJ/m2

PEKK 30% Glass Fiber Thermal properties

Melting point347–373°C
Glass temperature159–163°C
Heat deflection temperature 0.45MPa324–330°C
Heat deflection temperature 1.8MPa316–322°C
Vicat softening point324–330°C
Maximum service temperature233–287°C
Thermal conductivity0.422–0.458W/m.°C
Specific heat capacity1310–1340J/kg.°C
Thermal expansion coefficient15.6–16.4µstrain/°C
Thermal shock resistance725–803°C
Thermal distortion resistance0.0262–0.0288MW/m

PEKK Electrical properties

Electrical resistivity9249999999999999475712–10800000000000000000000µohm.cm
Electrical conductivity1.6e-20–1.86e-20%IACS
Dielectric constant (relative permittivity)3.17–3.43 
Dissipation factor (dielectric loss tangent)0.0035–0.0045 
Dielectric strength (dielectric breakdown)23–25MV/m

PEKK Magnetic properties

Magnetic typeNon-magnetic

PEKK Optical, aesthetic and acoustic properties

TransparencyOpaque
Acoustic velocity2790–2890m/s

PEKK Absorption & permeability

Water absorption @ 24 hrs0.063–0.077%

PEKK Processing properties

Polymer injection moldingAcceptable
Polymer extrusionLimited use
Polymer thermoformingUnsuitable
Linear mold shrinkage0.25 – 0.35 %
Melt temperature376 – 383 °C
Mold temperature132 – 249 °C
Molding pressure range103 – 138 MPa

PEKK Durability

Water (fresh)Excellent
Water (salt)Excellent
Weak acidsExcellent
Strong acidsUnacceptable
Weak alkalisExcellent
Strong alkalisExcellent
Organic solventsExcellent
Oils and fuelsExcellent
Oxidation at 500CUnacceptable
UV radiation (sunlight)Excellent
FlammabilitySelf-extinguishing