PEKK Unfilled Amorphous Material Data Sheet

PEKK Unfilled Amorphous (Polyetherketoneketone) Material Data Sheet

PEKK Unfilled Amorphous Overview

PEKK unfilled amorphous is a grade of polyetherketoneketone (PEKK), designated Polyetherketoneketone (unfilled, amorphous). This PEKK unfilled amorphous material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PEKK parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PEKK parts in-house and inspects them before shipment.

PEKK Designation

Polyetherketoneketone (unfilled, amorphous)
TradenamesOxpekk, Pyramid

PEKK Unfilled Amorphous Composition detail

Polymer100  %

PEKK Physical properties

Density1.27–1.29g/cm3

PEKK Unfilled Amorphous Mechanical properties

Young’s modulus3.36–3.53GPa
Specific stiffness2.62–2.77MN.m/kg
Yield strength (elastic limit)98–108MPa
Tensile strength85.1–94.1MPa
Specific strength76.5–84.5kN.m/kg
Elongation74–86% strain
Elongation at yield5–7% strain
Compressive modulus3.36–3.53GPa
Compressive strength97.8–108MPa
Flexural modulus3.29–3.46GPa
Flexural strength (modulus of rupture)135–141MPa
Shear modulus1.2–1.3GPa
Shear strength98–108MPa
Poisson’s ratio0.39–0.43 
Shape factor4.3
Hardness – Vickers25–28HV
Elastic stored energy (springs)1390–1690kJ/m3
Fatigue strength at 10^7 cycles34–37.6MPa

PEKK Impact & fracture properties

Impact strength, notched 23 °C4.32–5.28kJ/m2
Impact strength, unnotched 23 °C35–42kJ/m2

PEKK Unfilled Amorphous Thermal properties

Glass temperature146–163°C
Heat deflection temperature 0.45MPa136–153°C
Heat deflection temperature 1.8MPa133–149°C
Vicat softening point136–153°C
Maximum service temperature233–287°C
Thermal conductivity0.25  W/m.°C
Specific heat capacity1550–1580J/kg.°C
Thermal expansion coefficient75.1–78.9µstrain/°C
Thermal shock resistance365–412°C
Thermal distortion resistance0.00317–0.00333MW/m

PEKK Electrical properties

Electrical resistivity9250000000000000–10800000000000000µohm.cm
Electrical conductivity1.6e-14–1.86e-14%IACS
Dielectric constant (relative permittivity)3.17–3.43 
Dissipation factor (dielectric loss tangent)0.0035–0.0045 
Dielectric strength (dielectric breakdown)23–25MV/m

PEKK Magnetic properties

Magnetic typeNon-magnetic

PEKK Optical, aesthetic and acoustic properties

TransparencyTransparent
Acoustic velocity1620–1660m/s

PEKK Absorption & permeability

Water absorption @ 24 hrs0.18–0.22%

PEKK Processing properties

Polymer injection moldingAcceptable
Polymer extrusionLimited use
Polymer thermoformingUnsuitable
Linear mold shrinkage0.4 – 0.6 %

PEKK Durability

Water (fresh)Excellent
Water (salt)Excellent
Weak acidsExcellent
Strong acidsUnacceptable
Weak alkalisExcellent
Strong alkalisExcellent
Organic solventsExcellent
Oils and fuelsExcellent
Oxidation at 500CUnacceptable
UV radiation (sunlight)Excellent
FlammabilitySelf-extinguishing