Home » PEEK (Polyetheretherketone) » Modified PEEK 30% Carbon Fiber Material Data Sheet
Modified PEEK 30% Carbon Fiber (Polyetheretherketone) Material Data Sheet
Modified PEEK 30% Carbon Fiber Overview
Modified PEEK 30% carbon fiber is a grade of polyetheretherketone (PEEK), designated Modified poly(etheretherketone) (30% carbon fiber). This modified PEEK 30% carbon fiber material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PEEK parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PEEK parts in-house and inspects them before shipment.
Modified PEEK Designation
Modified poly(etheretherketone) (30% carbon fiber) Tradenames AvaSpire
Modified PEEK 30% Carbon Fiber Composition detail
Polymer 70 % Carbon (fiber) 30 %
Modified PEEK Physical properties
Modified PEEK 30% Carbon Fiber Mechanical properties
Young’s modulus 17.5 – 22.4 GPa Specific stiffness 12.3 – 15.8 MN.m/kg Yield strength (elastic limit) 145 – 160 MPa Tensile strength 178 – 199 MPa Specific strength 102 – 113 kN.m/kg Elongation 1.33 – 2.14 % strain Elongation at yield 1.3 – 2.1 % strain Compressive modulus 17.5 – 22.4 GPa Flexural modulus 15.1 – 19.3 GPa Flexural strength (modulus of rupture) 260 – 302 MPa Shear modulus 6.5 – 8.3 GPa Shear strength 90 – 99 MPa Poisson’s ratio 0.42 – 0.46 Shape factor 9.81 Hardness – Vickers 43 – 47 HV Elastic stored energy (springs) 502 – 683 kJ/m3 Fatigue strength at 10^7 cycles 71.6 – 79.1 MPa
Modified PEEK Impact & fracture properties
Impact strength, notched 23 °C 5.23 – 6.84 kJ/m2 Impact strength, unnotched 23 °C 53.2 – 64.2 kJ/m2
Modified PEEK 30% Carbon Fiber Thermal properties
Melting point 613 – 618 °C Glass temperature 150 – 168 °C Heat deflection temperature 0.45MPa 495 – 563 °C Heat deflection temperature 1.8MPa 483 – 549 °C Vicat softening point 495 – 563 °C Thermal conductivity 0.34 – 0.36 W/m.°C Specific heat capacity 1400 – 1420 J/kg.°C Thermal expansion coefficient 5 – 8.2 µstrain/°C Thermal shock resistance 913 – 1580 °C Thermal distortion resistance 0.0426 – 0.0701 MW/m
Modified PEEK Electrical properties
Electrical resistivity 10 – 100 µohm.cm Electrical conductivity 1.72 – 17.2 %IACS Dielectric constant (relative permittivity) 3.3 – 4 Dielectric strength (dielectric breakdown) 30 – 70 MV/m Galvanic potential 0.14 – 0.22 V
Modified PEEK Magnetic properties
Magnetic type Non-magnetic
Modified PEEK Optical, aesthetic and acoustic properties
Transparency Opaque Acoustic velocity 3500 – 3980 m/s
Modified PEEK Processing properties
Polymer injection molding Unsuitable Polymer extrusion Limited use Polymer thermoforming Unsuitable Melt temperature 366 – 388 °C Mold temperature 149 – 204 °C
Modified PEEK Durability
Water (fresh) Excellent Water (salt) Excellent Weak acids Excellent Strong acids Limited use Weak alkalis Excellent Strong alkalis Excellent Organic solvents Excellent Oils and fuels Excellent Oxidation at 500C Unacceptable UV radiation (sunlight) Excellent Flammability Self-extinguishing
PEEK Grades
Modified PEEK Carbon Filled Material Data Sheets
All PEEK Grades