Home » PEEK (Polyetheretherketone) » Modified PEEK 40% Glass Fiber Material Data Sheet
Modified PEEK 40% Glass Fiber (Polyetheretherketone) Material Data Sheet
Modified PEEK 40% Glass Fiber Overview
Modified PEEK 40% glass fiber is a grade of polyetheretherketone (PEEK), designated Modified poly(etheretherketone) (40% glass fiber). This modified PEEK 40% glass fiber material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PEEK parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PEEK parts in-house and inspects them before shipment.
Modified PEEK Designation
Modified poly(etheretherketone) (40% glass fiber) Tradenames AvaSpire
Modified PEEK 40% Glass Fiber Composition detail
Polymer 60 % Glass (fiber) 40 %
Modified PEEK Physical properties
Modified PEEK 40% Glass Fiber Mechanical properties
Young’s modulus 14.7 – 15.5 GPa Specific stiffness 8.91 – 9.4 MN.m/kg Yield strength (elastic limit) 147 – 162 MPa Tensile strength 181 – 201 MPa Specific strength 89 – 98.3 kN.m/kg Elongation 1.67 – 1.94 % strain Elongation at yield 1.7 – 1.9 % strain Compressive modulus 14.7 – 15.5 GPa Flexural modulus 14.4 – 15.2 GPa Flexural strength (modulus of rupture) 247 – 259 MPa Shear modulus 5.5 – 5.8 GPa Shear strength 84.5 – 93.5 MPa Poisson’s ratio 0.41 – 0.45 Shape factor 8.07 Hardness – Vickers 44 – 48 HV Elastic stored energy (springs) 715 – 870 kJ/m3 Fatigue strength at 10^7 cycles 72.6 – 80.2 MPa
Modified PEEK Impact & fracture properties
Impact strength, notched 23 °C 4.77 – 5.83 kJ/m2 Impact strength, unnotched 23 °C 53.1 – 64.9 kJ/m2
Modified PEEK 40% Glass Fiber Thermal properties
Melting point 610 – 626 °C Glass temperature 142 – 158 °C Heat deflection temperature 0.45MPa 565 – 579 °C Heat deflection temperature 1.8MPa 551 – 565 °C Vicat softening point 565 – 579 °C Thermal conductivity 0.304 – 0.316 W/m.°C Specific heat capacity 1200 – 1220 J/kg.°C Thermal expansion coefficient 14.8 – 15.2 µstrain/°C Thermal shock resistance 645 – 721 °C Thermal distortion resistance 0.0202 – 0.0212 MW/m
Modified PEEK Electrical properties
Electrical resistivity 1849999999999999995805696 – 2149999999999999937085440 µohm.cm Electrical conductivity 8.02e-23 – 9.32e-23 %IACS Dielectric constant (relative permittivity) 3.86 – 4.02 Dissipation factor (dielectric loss tangent) 8.24e-4 – 0.00408 Dielectric strength (dielectric breakdown) 15.4 – 16.6 MV/m
Modified PEEK Magnetic properties
Magnetic type Non-magnetic
Modified PEEK Optical, aesthetic and acoustic properties
Transparency Opaque Acoustic velocity 2980 – 3070 m/s
Modified PEEK Absorption & permeability
Water absorption @ 24 hrs 0.09 – 0.11 %
Modified PEEK Processing properties
Polymer injection molding Limited use Polymer extrusion Limited use Polymer thermoforming Unsuitable Linear mold shrinkage 0.3 – 0.8 % Melt temperature 370 – 395 °C Mold temperature 177 – 210 °C
Modified PEEK Durability
Water (fresh) Excellent Water (salt) Excellent Weak acids Excellent Strong acids Limited use Weak alkalis Excellent Strong alkalis Excellent Organic solvents Excellent Oils and fuels Excellent Oxidation at 500C Unacceptable UV radiation (sunlight) Excellent Flammability Self-extinguishing
PEEK Grades
Modified PEEK Glass Filled Material Data Sheets
All PEEK Grades
Modulus Metal Services