Home » PEEK (Polyetheretherketone) » Modified PEEK 30% Glass Fiber Material Data Sheet
Modified PEEK 30% Glass Fiber (Polyetheretherketone) Material Data Sheet
Modified PEEK 30% Glass Fiber Overview
Modified PEEK 30% glass fiber is a grade of polyetheretherketone (PEEK), designated Modified poly(etheretherketone) (30% glass fiber). This modified PEEK 30% glass fiber material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PEEK parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PEEK parts in-house and inspects them before shipment.
Modified PEEK Designation
Modified poly(etheretherketone) (30% glass fiber) Tradenames AvaSpire
Modified PEEK 30% Glass Fiber Composition detail
Polymer 70 % Glass (fiber) 30 %
Modified PEEK Physical properties
Modified PEEK 30% Glass Fiber Mechanical properties
Young’s modulus 9.85 – 10.1 GPa Specific stiffness 6.37 – 6.58 MN.m/kg Yield strength (elastic limit) 116 – 127 MPa Tensile strength 141 – 155 MPa Specific strength 75.2 – 82.6 kN.m/kg Elongation 2.6 – 3.2 % strain Elongation at yield 2.6 – 3.2 % strain Compressive modulus 9.85 – 10.1 GPa Flexural modulus 9.04 – 9.5 GPa Flexural strength (modulus of rupture) 222 – 239 MPa Shear modulus 3.7 – 3.8 GPa Shear strength 79 – 87 MPa Poisson’s ratio 0.41 – 0.45 Shape factor 7.18 Hardness – Vickers 34 – 38 HV Elastic stored energy (springs) 676 – 808 kJ/m3 Fatigue strength at 10^7 cycles 56.4 – 62.3 MPa
Modified PEEK Impact & fracture properties
Impact strength, notched 23 °C 9.51 – 12.2 kJ/m2 Impact strength, unnotched 23 °C 94 – 103 kJ/m2
Modified PEEK 30% Glass Fiber Thermal properties
Melting point 613 – 618 °C Glass temperature 149 – 167 °C Heat deflection temperature 0.45MPa 494 – 543 °C Heat deflection temperature 1.8MPa 482 – 530 °C Vicat softening point 494 – 543 °C Thermal conductivity 0.28 – 0.3 W/m.°C Specific heat capacity 1280 – 1310 J/kg.°C Thermal expansion coefficient 17 – 19 µstrain/°C Thermal shock resistance 631 – 728 °C Thermal distortion resistance 0.0151 – 0.0172 MW/m
Modified PEEK Electrical properties
Electrical resistivity 25000000000000000 – 100000000000000000 µohm.cm Electrical conductivity 1.72e-15 – 6.9e-15 %IACS Dielectric constant (relative permittivity) 3.3 – 4 Dissipation factor (dielectric loss tangent) 0.0013 – 0.0036 Dielectric strength (dielectric breakdown) 30 – 70 MV/m
Modified PEEK Magnetic properties
Magnetic type Non-magnetic
Modified PEEK Optical, aesthetic and acoustic properties
Transparency Opaque Acoustic velocity 2520 – 2560 m/s
Modified PEEK Absorption & permeability
Water absorption @ 24 hrs 0.18 – 0.22 % Water absorption @ sat 0.36 – 0.44 %
Modified PEEK Processing properties
Polymer injection molding Limited use Polymer extrusion Limited use Polymer thermoforming Unsuitable Linear mold shrinkage 0.3 – 0.9 % Melt temperature 366 – 388 °C Mold temperature 149 – 177 °C
Modified PEEK Durability
Water (fresh) Excellent Water (salt) Excellent Weak acids Excellent Strong acids Limited use Weak alkalis Excellent Strong alkalis Excellent Organic solvents Excellent Oils and fuels Excellent Oxidation at 500C Unacceptable UV radiation (sunlight) Excellent Flammability Self-extinguishing
PEEK Grades
Modified PEEK Glass Filled Material Data Sheets
All PEEK Grades
Modulus Metal Services
Manufacturing & Quality Services in Turkey