PEEK 40% Carbon Fiber Material Data Sheet

PEEK 40% Carbon Fiber (Polyetheretherketone) Material Data Sheet

PEEK 40% Carbon Fiber Overview

PEEK 40% carbon fiber is a grade of polyetheretherketone (PEEK), designated Polyetheretherketone (40% Carbon Fiber). This PEEK 40% carbon fiber material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PEEK parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PEEK parts in-house and inspects them before shipment.

PEEK Designation

Polyetheretherketone (40% Carbon Fiber)
TradenamesEdgetek, Hifill, Larpeek, LNP Thermocomp, Luvocom, RTP, Victrex

PEEK Typical uses

Aerospace applications, automotive applications, bearings, bushings, gears, general purpose, medical/healthcare applications, metal replacement, parts (engineering), pump parts, textile applications

PEEK 40% Carbon Fiber Composition detail

Polymer60  %
Carbon (fiber)40  %

PEEK Physical properties

Density1.44–1.47g/cm3

PEEK 40% Carbon Fiber Mechanical properties

Young’s modulus33.4–40GPa
Specific stiffness22.9–27.5MN.m/kg
Yield strength (elastic limit)241–269MPa
Tensile strength241–316MPa
Specific strength165–185kN.m/kg
Elongation1–1.5% strain
Elongation at yield1.3–1.4% strain
Compressive modulus21.4–22.5GPa
Compressive strength225–301MPa
Flexural modulus27.1–34GPa
Flexural strength (modulus of rupture)352–470MPa
Shear modulus12.1–12.7GPa
Shear strength126  MPa
Bulk modulus33.4–40GPa
Poisson’s ratio0.47
Shape factor10.5
Hardness – Vickers62–67HV
Hardness – Rockwell R118
Hardness – Shore D88–89 
Elastic stored energy (springs)773–1020kJ/m3
Fatigue strength at 10^7 cycles100–121MPa

PEEK Impact & fracture properties

Fracture toughness8.32–12MPa.m0.5
Toughness (G)1.93–3.86kJ/m2
Impact strength, notched 23 °C5–11kJ/m2
Impact strength, unnotched 23 °C40–86kJ/m2

PEEK 40% Carbon Fiber Thermal properties

Melting point343  °C
Glass temperature143  °C
Heat deflection temperature 0.45MPa300–339°C
Heat deflection temperature 1.8MPa288–349°C
Vicat softening point300  °C
Maximum service temperature235–250°C
Thermal conductivity2  W/m.°C
Specific heat capacity1800  J/kg.°C
Thermal expansion coefficient4–7.6µstrain/°C
Thermal shock resistance907–1760°C
Thermal distortion resistance0.263–0.5MW/m

PEEK Electrical properties

Electrical resistivity100000000000–1000000000000µohm.cm
Electrical conductivity1.72e-10–1.72e-9%IACS
Dielectric constant (relative permittivity)3.2–3.4 
Dissipation factor (dielectric loss tangent)0.005
Galvanic potential0.14–0.22V

PEEK Magnetic properties

Magnetic typeNon-magnetic

PEEK Optical, aesthetic and acoustic properties

TransparencyOpaque
Acoustic velocity4780–5250m/s
Mechanical loss coefficient (tan delta)0.0036–0.0053 

PEEK Absorption & permeability

Water absorption @ 24 hrs0.03–0.12%
Water absorption @ sat0.3  %
Humidity absorption @ sat0.3  %

PEEK Processing properties

Polymer injection moldingLimited use
Polymer extrusionLimited use
Polymer thermoformingLimited use
Linear mold shrinkage0.05 – 0.5 %
Melt temperature349 – 400 °C
Mold temperature121 – 260 °C
Molding pressure range68.9 – 207 MPa

PEEK Durability

Water (fresh)Excellent
Water (salt)Excellent
Weak acidsExcellent
Strong acidsUnacceptable
Weak alkalisExcellent
Strong alkalisExcellent
Organic solventsExcellent
Oxidation at 500CUnacceptable
UV radiation (sunlight)Excellent
FlammabilitySelf-extinguishing