PEEK 30% Carbon Fiber Material Data Sheet

PEEK 30% Carbon Fiber (Polyetheretherketone) Material Data Sheet

PEEK 30% Carbon Fiber Overview

PEEK 30% carbon fiber is a grade of polyetheretherketone (PEEK), designated Polyetheretherketone (30% Carbon Fiber). This PEEK 30% carbon fiber material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PEEK parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PEEK parts in-house and inspects them before shipment.

PEEK Designation

Polyetheretherketone (30% Carbon Fiber)
TradenamesGatone, Kebapeak, Ketaspire, Ketron, Larpeek, LNP Thermocomp, Luvocom, Schulatec, Vestakeep, Victrex

PEEK Typical uses

Wire covering, injection molded engineering products, film for flexible pcb, resin in fiber prepegs, aerospace applications, radiation environments, piping.

PEEK 30% Carbon Fiber Composition detail

Polymer70  %
Carbon (fiber)30  %

PEEK Physical properties

Density1.42–1.44g/cm3

PEEK 30% Carbon Fiber Mechanical properties

Young’s modulus20.7–25GPa
Specific stiffness14.5–17.5MN.m/kg
Yield strength (elastic limit)190–228MPa
Tensile strength190–228MPa
Specific strength133–159kN.m/kg
Elongation1–4% strain
Compressive modulus12.4–15GPa
Compressive strength172–240MPa
Flexural modulus17.2–23GPa
Flexural strength (modulus of rupture)276–335MPa
Shear modulus7.3–8.8GPa
Bulk modulus25.9–31.3GPa
Poisson’s ratio0.43–0.45 
Shape factor8.7
Hardness – Vickers49–55HV
Hardness – Rockwell M100–110 
Hardness – Rockwell R121–127 
Elastic stored energy (springs)784–1160kJ/m3
Fatigue strength at 10^7 cycles115–127MPa

PEEK Impact & fracture properties

Fracture toughness6.34–7.89MPa.m0.5
Toughness (G)1.76–2.75kJ/m2
Impact strength, notched 23 °C8.18–9.9kJ/m2
Impact strength, notched -30 °C7.27–8.8kJ/m2
Impact strength, unnotched 23 °C50–60.5kJ/m2
Impact strength, unnotched -30 °C50–60.5kJ/m2

PEEK 30% Carbon Fiber Thermal properties

Melting point322–346°C
Glass temperature143–157°C
Heat deflection temperature 0.45MPa295–354°C
Heat deflection temperature 1.8MPa288–321°C
Maximum service temperature260–280°C
Minimum service temperature-70–-50°C
Thermal conductivity0.87–0.97W/m.°C
Specific heat capacity1360–1410J/kg.°C
Thermal expansion coefficient10–15µstrain/°C
Thermal shock resistance591–944°C
Thermal distortion resistance0.0609–0.0924MW/m

PEEK Electrical properties

Electrical resistivity1000000–10000000µohm.cm
Electrical conductivity1.72e-5–1.72e-4%IACS
Galvanic potential0.14–0.22V

PEEK Magnetic properties

Magnetic typeNon-magnetic

PEEK Optical, aesthetic and acoustic properties

TransparencyOpaque
Acoustic velocity3800–4190m/s
Mechanical loss coefficient (tan delta)0.00431–0.00671 

PEEK Absorption & permeability

Water absorption @ 24 hrs0.06–0.12%

PEEK Processing properties

Polymer injection moldingLimited use
Polymer extrusionLimited use
Polymer thermoformingLimited use
Linear mold shrinkage0.05 – 1.4 %
Melt temperature309 – 427 °C
Mold temperature120 – 160 °C
Molding pressure range68.8 – 138 MPa

PEEK Durability

Water (fresh)Excellent
Water (salt)Excellent
Weak acidsExcellent
Strong acidsUnacceptable
Weak alkalisExcellent
Strong alkalisExcellent
Organic solventsExcellent
Oxidation at 500CUnacceptable
UV radiation (sunlight)Excellent
FlammabilitySelf-extinguishing