C18100 H.C. Copper, Cold Worked & Aged Material Data Sheet

C18100 H.C. Copper Material Data Sheet (Wrought, Cold Worked & Aged)

C18100 Cold Worked Aged Copper Overview

C18100 cold worked aged copper is a wrought high conductivity copper (UNS C18100, EN CW106C), known as h.c. copper. Condition: Precipitation hardened after cold working. This C18100 cold worked aged copper material data sheet covers its designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing and corrosion behaviour, and standards with similar compositions. Looking for C18100 copper parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined C18100 copper parts in-house and inspects them before shipment.

C18100 Designation

Copper Alloy: hc-CuCr1Zr(whp) (UNS C18100)
ConditionPrecipitation hardened after cold working
UNS numberC18100
EN nameCW106C
ISO nameCuCr1Zr

C18100 Typical uses

Heat sink material for the ITER.

C18100 Cold Worked Aged Copper Composition detail

Cr (chromium)0.4–1%
Cu (copper)98.7–99.5%
Mg (magnesium)0.03–0.06%
Zr (zirconium)0.08–0.2%

C18100 Physical properties

Density8.94–8.95g/cm3

C18100 Cold Worked Aged Copper Mechanical properties

Young’s modulus122–128GPa
Specific stiffness13.6–14.3MN.m/kg
Yield strength (elastic limit)320–420MPa
Tensile strength450–510MPa
Specific strength35.8–47kN.m/kg
Elongation13.5–16.5% strain
Compressive strength320–420MPa
Flexural modulus122–128GPa
Flexural strength (modulus of rupture)320–420MPa
Shear modulus45.1–47.4GPa
Bulk modulus132–138GPa
Poisson’s ratio0.34–0.35 
Shape factor23
Hardness – Vickers130–160HV
Elastic stored energy (springs)416–695kJ/m3
Fatigue strength at 10^7 cycles110–125MPa
Fatigue strength model (stress range)
Parameters: Stress Ratio = -1, Number of Cycles = 1e7cycles
102–134MPa

C18100 Impact & fracture properties

Fracture toughness33.3–40.4MPa.m0.5
Toughness (G)8.94–13kJ/m2

C18100 Cold Worked Aged Copper Thermal properties

Melting point1080  °C
Maximum service temperature300–350°C
Minimum service temperature-273  °C
Thermal conductivity390–398W/m.°C
Specific heat capacity383–387J/kg.°C
Thermal expansion coefficient16.8–16.9µstrain/°C
Thermal shock resistance152–200°C
Thermal distortion resistance23.1–23.6MW/m
Latent heat of fusion200–208kJ/kg

C18100 Electrical properties

Electrical resistivity2.09–2.19µohm.cm
Electrical conductivity78.7–82.5%IACS
Temperature dependence of resistivity5.2–5.4/°C
Galvanic potential-0.19–-0.11V

C18100 Magnetic properties

Magnetic typeNon-magnetic

C18100 Optical, aesthetic and acoustic properties

TransparencyOpaque
Acoustic velocity3690–3780m/s
Mechanical loss coefficient (tan delta)2.3e-5–3.9e-5 

C18100 Processing properties

Metal castingUnsuitable
Metal cold formingExcellent
Metal hot formingExcellent
Metal press formingExcellent
Metal deep drawingLimited use
Machining speed28.3 m/min
Weldability
Notes: Preheating and post weld heat treatment are not required
Poor

C18100 Durability

Water (fresh)Excellent
Water (salt)Excellent
Weak acidsAcceptable
Strong acidsUnacceptable
Weak alkalisExcellent
Strong alkalisExcellent
Organic solventsExcellent
Oxidation at 500CLimited use
UV radiation (sunlight)Excellent
Galling resistance (adhesive wear)Acceptable
FlammabilityNon-flammable

C18100 Cold Worked Aged Copper Corrosion resistance

Stress corrosion cracking
Note: Rated in ammoniacal; Other susceptible environments: Water, amine, dinitrogen tetroxide
Not susceptible

C18100 Notes

C18100 Cold Worked Aged Copper Other notes
(s)=soft; (1/2 h)=half hard; (h)=hard; (xh)=extra hard; (hr) = hot rolled; (w)=soln heat-trtd; (wh)=soln heat-trtd & work hdnd; (wp)=soln heat-trtd & precip hdnd; (whp)=precip hdnd after cold-wkng; (wph)=work hdnd after precip hdng.

C18100 Standards with similar compositions

Europe: CW106C to CEN EN 12163, CW106C to CEN EN 12165, CW106C to CEN EN 12167, CW106C to CEN EN 12420
Germany: 2.1293 to DIN, CuCrZr to DIN
Japan: CuCr1Zr to JIS Z3234, CuCrZr to JIS Z3234
USA: C18100, C18150, UNS C18100, UNS C18150
Tradenames: AMPCOLOY 972, BOLTOMET 819, CERRO CCZ, CMW 328, ELBRODUR HF, WIELAND-K60