| Designation | |
| UNS number | N10665 |
| US name | ASTM Grade N10655 |
| EN number | 2.4617 |
Durability: HASTELLOY B-2
| Water (fresh) | Excellent |
| Water (salt) | Excellent |
| Weak acids | Excellent |
| Strong acids | Excellent |
| Weak alkalis | Excellent |
| Strong alkalis | Excellent |
| Organic solvents | Excellent |
| Oxidation at 500°C | Excellent |
| UV radiation (sunlight) | Excellent |
| Galling resistance (adhesive wear) Notes :Bronze or zinc alloy dies should be used to minimize galling. | Limited use |
| Flammability | Non-flammable |
Corrosion resistance: HASTELLOY B-2
| Stress corrosion cracking Note: | Slightly susceptible Rated in chloride; Other susceptible environments: Hydroxide |
| Intergranular (weld line) corrosion | Excellent |
| Inorganic acids | Excellent |
| Organic acids | Good |
| Alkalis | Excellent |
| Humidity / water | Excellent |
| Sea water | Excellent |
| Sour oil and gas | Excellent |
MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey