HASTELLOY B-2 Thermal Properties (plate, Nickel-molybdenum alloy)

Designation
UNS numberN10665
US nameASTM Grade N10655
EN number2.4617

Thermal properties: HASTELLOY B-2

Melting point1350–1400°C
Maximum service temperature540–815°C
Minimum service temperature-273  °C
Thermal conductivity10–12.5W/m.°C
Specific heat capacity365–380J/kg.°C
Thermal expansion coefficient9.5–11.5µstrain/°C
Thermal shock resistance156–238°C
Thermal distortion resistance0.926–1.24MW/m
Latent heat of fusion285–300kJ/kg

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey