Designation: AISI 202
UNS number
S20200
US name
ASTM S20200
EN name
X12CrMnNiN18-9-5
EN number
1.4373
GB (Chinese) name
1Cr18Mn8Ni5N
Country
Equivalent / Similar Grade
Canada
202 to CSA G110.3, 202 to CSA G110.6
China
1Cr18Mn8Ni5N to GB 1220, 1Cr18Mn8Ni5N to GB 4237, 1Cr18Mn8Ni5N to GB/T 3280, 1Cr18Mn8Ni5N to GB/T 4239, 1Cr18Mn8Ni5N to GB/T 4356, 1Cr18Mn8Ni5N to GB/T 6725
Czech Republic
17460 to CSN 417460
India
TP202 to IS 11714/4, TP202 to IS 11714/5
International
A-3 to ISO 683-13
Japan
SUS202 to JIS G4303, SUS202 to JIS G4304, SUS202 to JIS G4305, SUS202 to JIS G4306, SUS202 to JIS G4307
South Korea
STS 202 to KS D 3706
UK
202S16 to BS 1554, 284S16 to BS 1449/2, X12CrMnNiN18-9-5 to BS EN 10088-1, X12CrMnNiN18-9-5 to BS EN 10088-2
USA
202 to ASTM A473, 202 to FED QQ-S-763F, 202 to FED QQ-S-766D, S20200 to ASTM A240/A240M, S20200 to ASTM A276, S20200 to ASTM A314-97, S20200 to ASTM A666, S20200 to ASTM A959, S20200 to SAE J405, TP202 to ASTM A213/A213M, TP202 to ASTM A249/A249M, UNS S20200, UNS S20281
Tradenames:
ALLEGHENY LUDLUM 204, ALLEGHENY LUDLUM TYPE 202, AMANOX 3965, JOSLYN STAINLESS TYPE 202, UNILOY 202