AISI 202 Stainless steel (Low nickel general purpose), austenitic | Weldability
Modulus Metal | Manufacturer Company in TURKEY: Sand Casting | Investment Casting | Foundry | CNC Machining | Press Bending | Laser Cutting | Welding | Plastics Injection Molding | Turkiye Weldability* Good Weldability – MIG Excellent Weldability – plasma Excellent Weldability – SAW Excellent Weldability – TIG Excellent Brazeability Fair *Notes: Preheating and post weld … Continue reading AISI 202 Stainless steel (Low nickel general purpose), austenitic | Weldability