AISI 202 Stainless steel (Low nickel general purpose), austenitic | Chemical Composition  

Modulus Metal | Manufacturer Company in TURKEY: Sand Casting | Investment Casting | CNC Machining | Press Bending | Laser Cutting | Welding | Plastics Injection Molding Composition detail % C (carbon)  0 – 0.15 % Cr (chromium)  17 – 19 % Fe (iron)  * 63.5 – 71.5 % Mn (manganese)  7.5 – 10 % … Continue reading AISI 202 Stainless steel (Low nickel general purpose), austenitic | Chemical Composition