Base Fe (Iron) : Fe/3.3-3.8C/2-3Si/<1.0Ni/0.2-0.5Mn/0.02-0.07Mg

| Material Standards with Similar Chemical Composition |
|---|
| NBN 830-02 FNG70-2 (Belgium) |
| NBN 830-02 FNG80-2 (Belgium) |
| GB 1348(88) QT 700-2 (China) |
| DS 11303 707 (Denmark) |
| DS 11303 708 (Denmark) |
| AFNOR NFA32201 FGS700-2 (France) |
| AFNOR NFA32201 FGS800-2 (France) |
| DIN WNr 0.7070 (Germany) |
| DIN 1693 GGG-70 (Germany) |
| IS 1865 SG700/2 (India) |
| IS 1865 SG800/2 (India) |
| UNI 4544 GS700-2 (Italy) |
| UNI 4544 GS800-2 (Italy) |
| JIS G5502(95) FCD70 Class 5 (Japan) |
| JIS G5502(95) FCD80 Class 6 (Japan) |
| NEN 2733 GN700-2 (Netherlands) |
| NEN 2733 GN800-2 (Netherlands) |
| NS 11301 NS11370 (Norway) |
| AS 1831(85) 700-2 (NSW Australia) |
| AS 1831(85) 800-2 (NSW Australia) |
| GOST 7293 VCh70 (Russian Federation) |
| GOST 7293 VCh80 (Russian Federation) |
| SABS 936 SG80 (South Africa) |
| ISO 1083(87) 700-2 (International) |
| ISO 1083(87) 800-2 (International) |
| BS 2789 700/2 (United Kingdom) |
| BS 2789 800/2 (United Kingdom) |
| ASTM A536(93) 100-70-03 (USA) |
| SAE J434 D7003 (USA) |