Base Fe (Iron) : Fe/3.3-3.8C/2-3Si/<1.0Ni/0.2-0.5Mn/0.02-0.07Mg

EN GSJ 700-2 as cast normalised Chemical Composition
EN GJS 700-2, as cast & normalized, Chemical Composition (Cast iron, nodular graphite)
Material Standards with Similar Chemical Composition
NBN 830-02 FNG70-2 (Belgium)
NBN 830-02 FNG80-2 (Belgium)
GB 1348(88) QT 700-2 (China)
DS 11303 707 (Denmark)
DS 11303 708 (Denmark)
AFNOR NFA32201 FGS700-2 (France)
AFNOR NFA32201 FGS800-2 (France)
DIN WNr 0.7070 (Germany)
DIN 1693 GGG-70 (Germany)
IS 1865 SG700/2 (India)
IS 1865 SG800/2 (India)
UNI 4544 GS700-2 (Italy)
UNI 4544 GS800-2 (Italy)
JIS G5502(95) FCD70 Class 5 (Japan)
JIS G5502(95) FCD80 Class 6 (Japan)
NEN 2733 GN700-2 (Netherlands)
NEN 2733 GN800-2 (Netherlands)
NS 11301 NS11370 (Norway)
AS 1831(85) 700-2 (NSW Australia)
AS 1831(85) 800-2 (NSW Australia)
GOST 7293 VCh70 (Russian Federation)
GOST 7293 VCh80 (Russian Federation)
SABS 936 SG80 (South Africa)
ISO 1083(87) 700-2 (International)
ISO 1083(87) 800-2 (International)
BS 2789 700/2 (United Kingdom)
BS 2789 800/2 (United Kingdom)
ASTM A536(93) 100-70-03 (USA)
SAE J434 D7003 (USA)

EN GJS 700 2, hardened & tempered, Chemical Composition (Cast iron, nodular graphite) | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

Base Fe (Iron) : Fe/3.3-3.8C/2-3Si/<1.0Ni/0.2-0.5Mn/0.02-0.07Mg

EN GSJ 700-2 Hardened Tempered Chemical Composition
EN GJS 700 2, hardened & tempered, Chemical Composition (Cast iron, nodular graphite)
Material Standards with Similar Chemical Composition
NBN 830-02 FNG70-2 (Belgium)
NBN 830-02 FNG80-2 (Belgium)
GB 1348(88) QT 700-2 (China)
DS 11303 707 (Denmark)
DS 11303 708 (Denmark)
AFNOR NFA32201 FGS700-2 (France)
AFNOR NFA32201 FGS800-2 (France)
DIN WNr 0.7070 (Germany)
DIN 1693 GGG-70 (Germany)
IS 1865 SG700/2 (India)
IS 1865 SG800/2 (India)
UNI 4544 GS700-2 (Italy)
UNI 4544 GS800-2 (Italy)
JIS G5502(95) FCD70 Class 5 (Japan)
JIS G5502(95) FCD80 Class 6 (Japan)
NEN 2733 GN700-2 (Netherlands)
NEN 2733 GN800-2 (Netherlands)
NS 11301 NS11370 (Norway)
AS 1831(85) 700-2 (NSW Australia)
AS 1831(85) 800-2 (NSW Australia)
GOST 7293 VCh70 (Russian Federation)
GOST 7293 VCh80 (Russian Federation)
SABS 936 SG80 (South Africa)
ISO 1083(87) 700-2 (International)
ISO 1083(87) 800-2 (International)
BS 2789 700/2 (United Kingdom)
BS 2789 800/2 (United Kingdom)
ASTM A536(93) 100-70-03 (USA)
SAE J434 D7003 (USA)