Base Fe (Iron) : Fe/3.3-3.8C/2-3Si/<1.0Ni/0.2-0.5Mn/0.02-0.07Mg

Material Standards with Similar Chemical Composition |
---|
NBN 830-02 FNG70-2 (Belgium) |
NBN 830-02 FNG80-2 (Belgium) |
GB 1348(88) QT 700-2 (China) |
DS 11303 707 (Denmark) |
DS 11303 708 (Denmark) |
AFNOR NFA32201 FGS700-2 (France) |
AFNOR NFA32201 FGS800-2 (France) |
DIN WNr 0.7070 (Germany) |
DIN 1693 GGG-70 (Germany) |
IS 1865 SG700/2 (India) |
IS 1865 SG800/2 (India) |
UNI 4544 GS700-2 (Italy) |
UNI 4544 GS800-2 (Italy) |
JIS G5502(95) FCD70 Class 5 (Japan) |
JIS G5502(95) FCD80 Class 6 (Japan) |
NEN 2733 GN700-2 (Netherlands) |
NEN 2733 GN800-2 (Netherlands) |
NS 11301 NS11370 (Norway) |
AS 1831(85) 700-2 (NSW Australia) |
AS 1831(85) 800-2 (NSW Australia) |
GOST 7293 VCh70 (Russian Federation) |
GOST 7293 VCh80 (Russian Federation) |
SABS 936 SG80 (South Africa) |
ISO 1083(87) 700-2 (International) |
ISO 1083(87) 800-2 (International) |
BS 2789 700/2 (United Kingdom) |
BS 2789 800/2 (United Kingdom) |
ASTM A536(93) 100-70-03 (USA) |
SAE J434 D7003 (USA) |