1.1141 Material Data Sheet : Non alloy special steels

1.1141 Material Data Sheet : Non alloy special steels

Material Number1.1141
Steel groupNon alloy special steels: Steels with special physical properties and structural, pressure vessel and engineering steels with average < 0,50%C
SymbolC15E; Ck 15
StandardsDIN EN 10084 : Case hardening steels.

International conformity: EN 10084

Predecessor document: DIN 17210 (09/1986)

DIN EN 10132-2 :Cold rolled narrow steel strip for heat treatment. Case hardening steels.

International conformity: EN 10132-2

DIN EN 10297-1: Seamless circular steel tubes for mechanical and general engineering purposes. Non-alloy and alloy steel tubes. Steels for case hardening (appendix)  

International conformity: EN 10297-1

Predecessor document: DIN 17204 (11/1990); DIN 1626 (10/1984); DIN 1629 (10/1984); DIN 1630 (10/1984)

Range of application:

Case hardening steels: Small machine components, levers, links, bushes, bolts, pins

1.1141 Material Composition

ElementMin/Max
C0.12 – 0.18
Si<=0.40
Mn0.30 – 0.60
P<=0.035
S<=0.035

1.1141 Standard Comparison

CountrySymbolMaterial No.Standard
AustriaC15E1.1141EN 10084 (04/2008) (AT)
AustriaC15E1.1141EN 10132~2 (02/2000) (AT)
AustriaC15E1.1141EN 10297~1 (02/2003) (AT)
BelgiumC15E1.1141EN 10084 (04/2008) (BE)
BelgiumC15E1.1141EN 10132~2 (02/2000) (BE)
BelgiumC15E1.1141EN 10297~1 (02/2003) (BE)
BulgariaC15E1.1141EN 10084 (04/2008) (BG)
BulgariaC15E1.1141EN 10132~2 (02/2000) (BG)
BulgariaC15E1.1141EN 10297~1 (02/2003) (BG)
ChinaU20152~1.1141T 699 (1999) (CN)
China15~1.1141T 699 (1999) (CN)
ChinaU20152~1.1141T 710 (1991) (CN)
China15~1.1141T 710 (1991) (CN)
China15~1.1141T 3078 (2008) (CN)
ChinaU20152~1.1141T 3078 (2008) (CN)
China15~1.1141T 3275 (1991) (CN)
ChinaU20152~1.1141T 3275 (1991) (CN)
China15~1.1141T 3522 (1983) (CN)
ChinaU20152~1.1141T 3522 (1983) (CN)
ChinaC22040~1.1141T 5676 (1985) (CN)
ChinaZG15 ~1.1141T 5676 (1985) (CN)
ChinaZG200~400~1.1141T 5676 (1985) (CN)
China15~1.1141T 8164 (1993) (CN)
ChinaU20152~1.1141T 8164 (1993) (CN)
China15~1.1141T 8749 (2008) (CN)
ChinaU20152~1.1141T 8749 (2008) (CN)
ChinaU20152~1.1141T 13237 (1991) (CN)
China15~1.1141T 13237 (1991) (CN)
ChinaU20152~1.1141T 13795 (1992) (CN)
China15~1.1141T 13795 (1992) (CN)
ChinaU20152~1.1141T 13796 (1992) (CN)
China15~1.1141T 13796 (1992) (CN)
CyprusC15E1.1141EN 10084 (04/2008) (CY)
CyprusC15E1.1141EN 10132~2 (02/2000) (CY)
CyprusC15E1.1141EN 10297~1 (02/2003) (CY)
Czech Republic12020~1.1141412020 (1987) (CZ)
Czech Republic12023~1.1141412023 (1987) (CZ)
Czech RepublicC15E1.1141EN 10084 (04/2008) (CZ)
Czech RepublicC15E1.1141EN 10132~2 (02/2000) (CZ)
Czech RepublicC15E1.1141EN 10297~1 (02/2003) (CZ)
DenmarkC15E1.1141EN 10084 (04/2008) (DK)
DenmarkC15E1.1141EN 10132~2 (02/2000) (DK)
DenmarkC15E1.1141EN 10297~1 (02/2003) (DK)
EstoniaC15E1.1141EN 10084 (04/2008) (EE)
EstoniaC15E1.1141EN 10132~2 (02/2000) (EE)
EstoniaC15E1.1141EN 10297~1 (02/2003) (EE)
EuropeC15E1.114110084 (04/2008) (EUR)
EuropeC15E1.114110132~2 (02/2000) (EUR)
EuropeC15E1.114110297~1 (02/2003) (EUR)
FinlandC15E1.1141EN 10084 (04/2008) (Fl)
FinlandC15E1.1141EN 10132~2 (02/2000) (Fl)
FinlandC15E1.1141EN 10297~1 (02/2003) (Fl)
FranceXC 18~1.1141A 35~566 (1983) (FR)
FranceC18RR~1.1141A 36~102 (1993) (FR)
Francexc 18 ~1.1141A 36~102 (1993) (FR)
FranceXC15~1.1141A 37~503 (1987) (FR)
FranceC15E1.1141EN 10084 (04/2008) (FR)
FranceC15E1.1141EN 10132~2 (02/2000) (FR)
FranceC15E1.1141EN 10297~1 (02/2003) (FR)
FranceXC 15~1.1141Non standardized steels (FR)
Francexc 18 1.1141A 35~551 (1984) withdrawn (FR)
Great BritainC15E1.1141EN 10084 (04/2008) (GB)
Great BritainC15E1.1141EN 10132~2 (02/2000) (GB)
Great BritainC15E1.1141EN 10297~1 (02/2003) (GB)
Great Britain080 A 15 1.1141970 Part 1 (1996) withdrawn (GB)
Great Britain080 M 15 1.1141970 Part 1 (1996) withdrawn (GB)
Great BritainEn 32 C 1.1141970 Part 1 (1996) withdrawn (GB)
GreeceC15E1.1141EN 10084 (04/2008) (GR)
GreeceC15E1.1141EN 10132~2 (02/2000) (GR)
GreeceC15E1.1141EN 10297~1 (02/2003) (GR)
HungaryC15E1.1141EN 10084 (04/2008) (HU)
HungaryC15E1.1141EN 10132~2 (02/2000) (HU)
HungaryC15E1.1141EN 10297~1 (02/2003) (HU)
Hungaryc 15 1.114131 (1985) withdrawn (HU)
IcelandC15E1.1141EN 10084 (04/2008) (IS)
IcelandC15E1.1141EN 10132~2 (02/2000) (IS)
IcelandC15E1.1141EN 10297~1 (02/2003) (IS)
IndiaC14 ~1.11411570 Part 2 Sec 1 (1979) (IN)
IndiaC15 ~1.11411570 Part 2 Sec 1 (1979) (IN)
India14C6~1.11411570 Part 2 Sec 1 (1979) (IN)
India15C4~1.11411570 Part 2 Sec 1 (1979) (IN)
India14C6~1.11411570 Part II (1979) (IN)
India15C4~1.11411570 Part II (1979) (IN)
IndiaC15 ~1.11411570 Part II (1979) (IN)
IndiaC14 ~1.11411570 Part II (1979) (IN)
India1(IS 1875)~1.11411875 (1992) (IN)
India14C6~1.11411875 (1992) (IN)
India1(IS 2004)~1.11412004 (1991) (IN)
India14C6~1.11412004 (1991) (IN)
India15C8~1.11414432 (1988) (IN)
India14C6~1.11415489 (1975) (IN)
India15C4~1.114111169 Part 1 (1984) (IN)
IndiaC14 ~1.114111169 Part 1 (1984) (IN)
IndiaC14 ~1.114111169 Part 1 (1984) (IN)
India14C6~1.114111169 Part 1 (1984) (IN)
India14C6~1.114111169 Part 1 (1984) (IN)
IndiaC15 ~1.114111169 Part 1 (1984) (IN)
IndiaC15~1.114111952 (1986) (IN)
IrelandC15E1.1141EN 10084 (04/2008) (IE)
IrelandC15E1.1141EN 10132~2 (02/2000) (IE)
IrelandC15E1.1141EN 10297~1 (02/2003) (IE)
ISOC15E4~1.1141683~11(1987) (ISO)
ISOCE 15E4~1.11414954 (1993) (ISO)
ISOS15C~1.114110384 (2008) (ISO)
ItalyC15E1.1141EN 10084 (04/2008) (IT)
ItalyC15E1.1141EN 10132~2 (02/2000) (IT)
ItalyC15E1.1141EN 10297~1 (02/2003) (IT)
Italy1c 151.11418373 (1982) withdrawn (IT)
Italyc 151.11418550 (1984) withdrawn (IT)
Japans 15 c~1.1141G 4051 (2005) (JP)
JapanS 15 CK~1.1141G 4051 (2005) (JP)
LatviaC15E1.1141EN 10084 (04/2008) (LV)
LatviaC15E1.1141EN 10132~2 (02/2000) (LV)
LatviaC15E1.1141EN 10297~1 (02/2003) (LV)
LithuaniaC15E1.1141EN 10084 (04/2008) (LT)
LithuaniaC15E1.1141EN 10132~2 (02/2000) (LT)
LithuaniaC15E1.1141EN 10297~1 (02/2003) (LT)
LuxemburgC15E1.1141EN 10084 (04/2008) (LU)
LuxemburgC15E1.1141EN 10132~2 (02/2000) (LU)
LuxemburgC15E1.1141EN 10297~1 (02/2003) (LU)
MaltaC15E1.1141EN 10084 (04/2008) (MT)
MaltaC15E1.1141EN 10132~2 (02/2000) (MT)
MaltaC15E1.1141EN 10297~1 (02/2003) (MT)
NetherlandsC15E1.1141EN 10084 (04/2008) (NL)
NetherlandsC15E1.1141EN 10132~2 (02/2000) (NL)
NetherlandsC15E1.1141EN 10297~1 (02/2003) (NL)
NorwayC15E1.1141EN 10084 (04/2008) (NO)
NorwayC15E1.1141EN 10132~2 (02/2000) (NO)
NorwayC15E1.1141EN 10297~1 (02/2003) (NO)
Norway131151.114113101withdrawn (NO)
PolandC15E1.1141EN 10084 (04/2008) (PL)
PolandC15E1.1141EN 10132~2 (02/2000) (PL)
PolandC15E1.1141EN 10297~1 (02/2003) (PL)
PortugalC15E1.1141EN 10084 (04/2008) (PT)
PortugalC15E1.1141EN 10132~2 (02/2000) (PT)
PortugalC15E1.1141EN 10297~1 (02/2003) (PT)
Republic of KoreaSM 15 C~1.1141D 3752 (2007) (KR)
Republic of KoreaSM 15 CK~1.1141D 3752 (2007) (KR)
RomaniaOLC 15A~1.11418580 (1988) (RO)
RumaniaC15E1.1141EN 10084 (04/2008) (RO)
RumaniaC15E1.1141EN 10132~2 (02/2000) (RO)
RumaniaC15E1.1141EN 10297~1 (02/2003) (RO)
Russia15~1.11411050 (1988) (RU)
SerbiaC15E1.1141EN 10084 (04/2008) (CS)
SerbiaC15E1.1141EN 10132~2 (02/2000) (CS)
SerbiaC15E1.1141EN 10297~1 (02/2003) (CS)
SerbiaC12211.1141C.89.020 (1989) withdrawn (CS)
Slovakia12020~1.1141412020 (1987) (SK)
Slovakia12023~1.1141412023 (1987) (SK)
SlovakiaC15E1.1141EN 10084 (04/2008) (SK)
SlovakiaC15E1.1141EN 10132~2 (02/2000) (SK)
SlovakiaC15E1.1141EN 10297~1 (02/2003) (SK)
SloveniaC15E1.1141EN 10084 (04/2008) (SL)
SloveniaC15E1.1141EN 10132~2 (02/2000) (SL)
SloveniaC15E1.1141EN 10297~1 (02/2003) (SL)
SpainC15E1.1141EN 10084 (04/2008) (ES)
SpainC15E1.1141EN 10132~2 (02/2000) (ES)
SpainC15E1.1141EN 10297~1 (02/2003) (ES)
Spainc 16 k1.114136013 (1976/1979) withdrawn (ES)
SpainF.15111.114136013 (1976/1979) withdrawn (ES)
SwedenC15E1.1141EN 10084 (04/2008) (SE)
SwedenC15E1.1141EN 10132~2 (02/2000) (SE)
SwedenC15E1.1141EN 10297~1 (02/2003) (SE)
Sweden1370~1.1141141370withdrawn (SE)
Switzer landC15E1.1141EN 10084 (04/2008) (CH)
Switzer landC15E1.1141EN 10132~2 (02/2000) (CH)
SwitzerlandC15E1.1141EN 10297~1 (02/2003) (CH)
TurkeyC15E1.1141EN 10084 (04/2008) (TR)
TurkeyC15E1.1141EN 10132~2 (02/2000) (TR)
TurkeyC15E1.1141EN 10297~1 (02/2003) (TR)
U.S.A.AMS~S~11310 (CS 1017)~1.1141
U.S.A.(AMS)   5060J (AMS)~1.1141
U.S.A.G10150 (UNS)~1.1141
U.S.A.G10170 (UNS)~1.1141
U.S.A.1015 (AISI)~1.1141
U.S.A.1017 (AISI)~1.1141
U.S.A.A 29 (1015) (AS M)~1.1141A 29~05(US)
U.S.A.A 29 (1017) (AS M)~1.1141A29~05(US)
U.S.A.A 108 (1015) (AS M)~1.1141A 108~07(US)
U.S.A.A 108 (1017) (AS M)~1.1141A 108~07(US)
U.S.A.A 125 (1015) (AS M)~1.1141A 125~96 (07)(US)
U.S.A.A 125 (1017) (AS M)~1.1141A 125~96 (07)(US)
U.S.A.A 510 (1015) (AS M)~1.1141A 510~07/06(US)
U.S.A.A 510 (1017) (AS M)~1.1141A 510~07/06(US)
U.S.A.A 512 (1015) (AS M)~1.1141A 512~06(US)
U.S.A.A 513 (1015) (AS M)~1.1141A 513~08(US)
U.S.A.A 513 (1017) (AS M)~1.1141A 513~08(US)
U.S.A.A 519 (1015) (AS M)~1.1141A 519~06(US)
U.S.A.A 519 (1017) (AS M)~1.1141A 519~06(US)
U.S.A.A 521 (1015)(AS M)~1.1141A 521~06(US)
U.S.A.A 521 (1017)(AS M)~1.1141A 521~06(US)
U.S.A.A 568 (1015) (AS M)~1.1141A 568~07(US)
U.S.A.A 568 (1017) (AS M)~1.1141A 568~07(US)
U.S.A.A 576 (1015) (AS M)~1.1141A 576~90 (06)(US)
U.S.A.A 576 (1017) (AS M)~1.1141A 576~90 (06)(US)
U.S.A.A 635 (1015) (AS M)~1.1141A 635~07(US)
U.S.A.A 635 (1017) (AS M)~1.1141A 635~07(US)
U.S.A.A 659 (1015) (AS M)~1.1141A 659~06(US)
U.S.A.A 659 (1017) (AS M)~1.1141A 659~06(US)
U.S.A.A 689 (1015) (AS M)~1.1141A 689~97 (07)(US)
U.S.A.A 689 (1017) (AS M)~1.1141A 689~97 (07)(US)
U.S.A.A 711 (1015)(AS M)~1.1141A 711~07(US)
U.S.A.A 711 (1017) (AS M)~1.1141A 711~07(US)
U.S.A.A 787 (1015) (AS M)~1.1141A 787~05(US)
U.S.A.A 787 (1017) (AS M)~1.1141A 787~05(US)
U.S.A.A 794 (1015) (AS M)~1.1141A 794~06(US)
U.S.A.A 794 (1017) (AS M)~1.1141A 794~06(US)
U.S.A.A 830 (1015) (AS M)~1.1141A 830~06(US)
U.S.A.A 830 (1017) (AS M)~1.1141A 830~06(US)
U.S.A.A 853 (1015) (AS M)~1.1141A 853~04(US)
U.S.A.A 1018 (CS 1017) (AS M)~1.1141A 1018~08(US)
U.S.A.A 1018 (CS 1015) (ASTM)~1.1141A 1018-08(US)
U.S.A.1015 (SAE)~1.1141J 403 (2001) (US)
U.S.A.1017 (SAE)~1.1141J 403 (2001) (US)

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey, Additive Manufacturing and 3D Printing in Turkey, Quality Enginering and Inspection Service in Turkey, Manufacturing Inspection Service in Turkey, Quality Engineering and Supplier Quality Engineering Service in Turkey, Supplier Quality Control and Inspection Service in Turkey, Resident Engineering Services in Turkey