1.1126 Material Data Sheet : Non alloy special steels
| Material Number | 1.1126 |
| Steel group | Non alloy special steels: Steels with special physical properties and structural, pressure vessel and engineering steels with average < 0,50%C |
| Symbol | C15D2 |
| Standards | DIN EN 10016-4 (04/1995): Non-alloy wire rod for drawing and/or cold rolling. Specific requirements for rod for special applications. International conformity: EN 10016-4 (1994); ISO 16120-4 (2001) Predecessor document: DIN 17140-2 (04/1988) Successor document: E DIN EN ISO 16120-4 (12/2009) |
1.1126 Material Composition
| Element | Min/Max |
|---|---|
| C | 0.13 – 0.17 |
| Si | <=0.30 |
| Mn | 0.30 – 0.50 |
| P | <=0.020 |
| S | <=0.025 |
| Al | <=0.0100 |
| Cr | <=0.10 |
| Cu | <=0.15 |
| Mo | <=0.05 |
| N | <=0.007 |
| Ni | <=0.10 |
| Note: | (Cu + Ni + Cr) <= 0,30% Cu + Sn) <= 0,15% |
1.1126 Standard Comparison
| Country | Symbol | Material No. | Standard |
|---|---|---|---|
| Austria | C15D2 | 1.1126 | EN 10016-4 (12/ 1994) (AT) |
| Belgium | C15D2 | 1.1126 | EN 10016-4 (12/ 1994) (BE) |
| Bulgaria | C15D2 | 1.1126 | EN 10016-4 (12/ 1994) (BG) |
| Cyprus | C15D2 | 1.1126 | EN 10016-4 (12/ 1994) (CY) |
| Czech Republic | C15D2 | 1.1126 | EN 10016-4 (12/ 1994) (CZ) |
| Denmark | C15D2 | 1.1126 | EN 10016-4 (12/ 1994) (DK) |
| Estonia | C15D2 | 1.1126 | EN 10016-4 (12/ 1994) (EE) |
| Europe | C15D2 | 1.1126 | 10016-4 (12/ 1994) (EUR) |
| Finland | C15D2 | 1.1126 | EN 10016-4 (12/ 1994) (Fl) |
| France | C15D2 | 1.1126 | EN 10016-4 (12/ 1994) (FR) |
| Great Britain | C15D2 | 1.1126 | EN 10016-4 (12/ 1994) (GB) |
| Greece | C15D2 | 1.1126 | EN 10016-4 (12/ 1994) (GR) |
| Hungary | C15D2 | 1.1126 | EN 10016-4 (12/ 1994) (HU) |
| Iceland | C15D2 | 1.1126 | EN 10016-4 (12/ 1994) (IS) |
| Ireland | C15D2 | 1.1126 | EN 10016-4 (12/ 1994) (IE) |
| ISO | C15D2 | ~1.1126 | 16120-4 (2001) (ISO) |
| Italy | C15D2 | 1.1126 | EN 10016-4 (12/ 1994) (IT) |
| Latvia | C15D2 | 1.1126 | EN 10016-4 (12/ 1994) (LV) |
| Lithuania | C15D2 | 1.1126 | EN 10016-4 (12/ 1994) (LT) |
| Luxemburg | C15D2 | 1.1126 | EN 10016-4 (12/ 1994) (LU) |
| Malta | C15D2 | 1.1126 | EN 10016-4 (12/ 1994) (MT) |
| Netherlands | C15D2 | 1.1126 | EN 10016-4 (12/ 1994) (NL) |
| Norway | C15D2 | 1.1126 | EN 10016-4 (12/ 1994) (NO) |
| Poland | C15D2 | 1.1126 | EN 10016-4 (12/ 1994) (PL) |
| Portugal | C15D2 | 1.1126 | EN 10016-4 (12/ 1994) (PT) |
| Rumania | C15D2 | 1.1126 | EN 10016-4 (12/ 1994) (RO) |
| Serbia | C15D2 | 1.1126 | EN 10016-4 (12/ 1994) (CS) |
| Slovakia | C15D2 | 1.1126 | EN 10016-4 (12/ 1994) (SK) |
| Slovenia | C15D2 | 1.1126 | EN 10016-4 (12/ 1994) (SL) |
| Spain | C15D2 | 1.1126 | EN 10016-4 (12/ 1994) (ES) |
| Sweden | C15D2 | 1.1126 | EN 10016-4 (12/ 1994) (SE) |
| Switzerland | C15D2 | 1.1126 | EN 10016-4 (12/ 1994) (CH) |
| Turkey | C15D2 | 1.1126 | EN 10016-4 (12/ 1994) (TR) |
MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey, Additive Manufacturing and 3D Printing in Turkey, Quality Enginering and Inspection Service in Turkey, Manufacturing Inspection Service in Turkey, Quality Engineering and Supplier Quality Engineering Service in Turkey, Supplier Quality Control and Inspection Service in Turkey, Resident Engineering Services in Turkey