EN GJS 800 2, as cast & normalized, Chemical Composition (Cast iron, nodular graphite) | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

Base Fe (Iron) : Fe/3.4-3.8C/2-2.8Si/<2.0Ni/<1.0Mo/0.2-0.6Mn/0.02-0.07Mg

EN GSJ 800-2 as cast normalized Chemical Composition
EN GJS 800 2, as cast & normalized, Chemical Composition (Cast iron, nodular graphite)
Material Standards with Similar Chemical Composition
GB 1348(88) QT 800-2 (China)
GB 1348(88) QT 900-2 (China)
AFNOR NFA32201 FGS900-2 (France)
DIN WNr 0.7080 (Germany)
DIN 1693 GGG-80 (Germany)
NS 11301 NS11380 (Norway)
GOST 7293 VCh100 (Russian Federation)
ISO 1083(87) 900-2 (International)
BS 2789 900/2 (United Kingdom)
ASTM A536(93) 120-90-02 (USA)

EN GJS 800 2, hardened & tempered, Chemical Composition (Cast iron, nodular graphite) | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

Base Fe (Iron) : Fe/3.4-3.8C/2-2.8Si/<2.0Ni/<1.0Mo/0.2-0.6Mn/0.02-0.07Mg

EN GSJ 800-2 Hardened Tempered Chemical Composition
EN GJS 800 2, hardened & tempered, Chemical Composition (Cast iron, nodular graphite)
Material Standards with Similar Chemical Composition
GB 1348(88) QT 800-2 (China)
GB 1348(88) QT 900-2 (China)
AFNOR NFA32201 FGS900-2 (France)
DIN WNr 0.7080 (Germany)
DIN 1693 GGG-80 (Germany)
NS 11301 NS11380 (Norway)
GOST 7293 VCh100 (Russian Federation)
ISO 1083(87) 900-2 (International)
BS 2789 900/2 (United Kingdom)
ASTM A536(93) 120-90-02 (USA)

EN GJS 900 2, as cast & normalized, Chemical Composition (Cast iron, nodular graphite) | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

Base Fe (Iron) : Fe/3.2-4.1C/1.8-2.8Si/<0.8Mn/<0.1P/<0.03S

EN GSJ 900-2 as cast normalised Chemical Composition
EN GJS 900 2, as cast & normalized, Chemical Composition (Cast iron, nodular graphite)
Material Standards with Similar Chemical Composition
GB 1348(88) QT 800-2 (China)
GB 1348(88) QT 900-2 (China)
AFNOR NFA32201 FGS900-2 (France)
DIN WNr 0.7080 (Germany)
DIN 1693 GGG-80 (Germany)
NS 11301 NS11380 (Norway)
GOST 7293 VCh100 (Russian Federation)
ISO 1083(87) 900-2 (International)
BS 2789 900/2 (United Kingdom)
ASTM A536(93) 120-90-02 (USA)

EN GJS 900 2, hardened & tempered, Chemical Composition (Cast iron, nodular graphite) | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

Base Fe (Iron) : Fe/3.2-4.1C/1.8-2.8Si/<0.8Mn/<0.1P/<0.03S

EN GSJ 900-2 Hardened Tempered Chemical Composition
EN GJS 900 2, hardened & tempered, Chemical Composition (Cast iron, nodular graphite)
Material Standards with Similar Chemical Composition
GB 1348(88) QT 800-2 (China)
GB 1348(88) QT 900-2 (China)
AFNOR NFA32201 FGS900-2 (France)
DIN WNr 0.7080 (Germany)
DIN 1693 GGG-80 (Germany)
NS 11301 NS11380 (Norway)
GOST 7293 VCh100 (Russian Federation)
ISO 1083(87) 900-2 (International)
BS 2789 900/2 (United Kingdom)
ASTM A536(93) 120-90-02 (USA)