EN GJS 800-2 hardened & tempered, nodular graphite, Mechanical Properties Young’s modulus 168 – 176 GPa Flexural modulus * 168 – 176 GPa Shear modulus 65 – 70 GPa Bulk modulus 121 – 134 GPa Poisson’s ratio 0.27 – 0.28 Shape factor 18 Yield strength (elastic limit) 630 – 710 MPa Tensile strength 800 – … Continue reading EN GJS 800-2 hardened & tempered, nodular graphite, Mechanical Properties | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY