Cast iron, gray, flake graphite, EN GJL 200 Equivalent Grades | Modulus Metal | Supplier | Foundry | Castings Products | in TURKEY

Gray Cast Iron Microstucture Foundry Supplier Parts Products Exporter Manufacturing in Turkey

EN GJL 200 Equivalent Grades

Standard/OrganizationDesignation
BS EN 1561:1997EN GJL 200
BS 1542:1990BS grade 200
UNS NumberF12101
DIN 1691GG20 (Germany)

Standards with similar compositions:

NBN 83001 FGG20 (Belgium)
GB 9439(88) HT 200 (China)
DS 11301 GG20 (Denmark)
AFNOR NFA32101 FGL200
DIN 1691 GG15 (Germany)
IS 210 FG200 (India)
UNI 5007 G20 (Italy)
JIS G5501(95) FC200 (Japan)
NEN 6002A GG20 (Netherlands)
NS 722 SjG20 (Norway)
NS 722 SjG250 (Norway)
GOST 1412 SCh20 (Russian)
SABS 1034 200 (South Africa)
ISO 185(88) 200 (International)
BS 1452 200 (United Kingdom)
ASME SA278 30 (USA)
ASTM A126(95) B (USA)
ASTM A278(93) 30 (USA)
ASTM A278M(93) 200 (USA)
ASTM A48(94) 30A (USA)
ASTM A48(94) 30B (USA)
ASTM A48(94) 30C (USA)
ASTM A48(94) 30S (USA)