EN GJS 400 18U Chemical Composition (Cast iron, nodular graphite) | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

Base Fe (Iron) : Fe/3.4-4C/2-2.8Si/0.2-0.6Mn/0.02-0.07Mg

EN GJS 400 18U Chemical Composition
EN GJS 400 18U Chemical Composition (Cast iron, nodular graphite)
Material Standards with Similar Chemical Composition
NBN 830-02 FNG38-17 (Belgium)
GB 1348(88) QT 400-15 (China)
GB 1348(88) QT 400-18 (China)
DS 11303 715 (Denmark)
DS 11303 716 (Denmark)
AFNOR NFA32201 FGS350-22 (France)
AFNOR NFA32201 FGS350-22L (France)
AFNOR NFA32201 FGS400-15 (France)
AFNOR NFA32201 FGS400-18 (France)
AFNOR NFA32201 FGS400-18L (France)
DIN WNr 0.7040 (Germany)
DIN WNr 0.7043 (Germany)
DIN 1693 GGG-35.3 (Germany)
DIN 1693 GGG-40 (Germany)
DIN 1693 GGG-40.3 (Germany)
IS 1865 SG370/17 (India)
UNI 4544 GS370-17 (Italy)
JIS G5502(95) FCD37 Class 0 (Japan)
NEN 2733 GN350-22L (Netherlands)
NEN 2733 GN400-15 (Netherlands)
NEN 2733 GN400-18L (Netherlands)
NS 11301 NS11335 (Norway)
NS 11301 NS11338 (Norway)
NS 11301 NS11342 (Norway)
AS 1831(85) 370-17 (NSW Australia)
GOST 7293 VCh35 (Russian Federation)
GOST 7293 VCh40 (Russian Federation)
SABS 936 SG38 (South Africa)
SIS 140717 0717-00 (Sweden)
SIS 140717 0717-02 (Sweden)
SIS 140717 0717-15 (Sweden)
ISO 1083(87) 350-22 (International)
ISO 1083(87) 350-22L (International)
ISO 1083(87) 400-15 (International)
ISO 1083(87) 400-18 (International)
ISO 1083(87) 400-18L (International)
BS 2789 350/22 (United Kingdom)
BS 2789 350/22L40 (United Kingdom)
BS 2789 400/18 (United Kingdom)
BS 2789 400/18L20 (United Kingdom)
ASME SA395 60-40-18 (USA)
ASTM A356(84) 60-40-18 (USA)
ASTM A395/A395(98) 60-40-18 (USA)
ASTM A536(93) 60-40-18 (USA)
MIL-C-24707/5(89) 60-45-15 (USA)
SAE J434 D4018 (USA)

EN GJS 400 18 LT Chemical Composition (Cast iron, nodular graphite) | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

Base Fe (Iron) : Fe/3.2-4.1C/2-2.5Si/<0.8Mn/<0.04P/<0.03S

EN-GJS-400-18-LT-Chemical-Composition
EN GJS 400 18 LT Chemical Composition (Cast iron, nodular graphite)
Material Standards with Similar Chemical Composition
NBN 830-02 FNG38-17 (Belgium)
GB 1348(88) QT 400-15 (China)
GB 1348(88) QT 400-18 (China)
DS 11303 715 (Denmark)
DS 11303 716 (Denmark)
AFNOR NFA32201 FGS350-22 (France)
AFNOR NFA32201 FGS350-22L (France)
AFNOR NFA32201 FGS400-15 (France)
AFNOR NFA32201 FGS400-18 (France)
AFNOR NFA32201 FGS400-18L (France)
DIN WNr 0.7040 (Germany)
DIN WNr 0.7043 (Germany)
DIN 1693 GGG-35.3 (Germany)
DIN 1693 GGG-40 (Germany)
DIN 1693 GGG-40.3 (Germany)
IS 1865 SG370/17 (India)
UNI 4544 GS370-17 (Italy)
JIS G5502(95) FCD37 Class 0 (Japan)
NEN 2733 GN350-22L (Netherlands)
NEN 2733 GN400-15 (Netherlands)
NEN 2733 GN400-18L (Netherlands)
NS 11301 NS11335 (Norway)
NS 11301 NS11338 (Norway)
NS 11301 NS11342 (Norway)
AS 1831(85) 370-17 (NSW Australia)
GOST 7293 VCh35 (Russian Federation)
GOST 7293 VCh40 (Russian Federation)
SABS 936 SG38 (South Africa)
SIS 140717 0717-00 (Sweden)
SIS 140717 0717-02 (Sweden)
SIS 140717 0717-15 (Sweden)
ISO 1083(87) 350-22 (International)
ISO 1083(87) 350-22L (International)
ISO 1083(87) 400-15 (International)
ISO 1083(87) 400-18 (International)
ISO 1083(87) 400-18L (International)
BS 2789 350/22 (United Kingdom)
BS 2789 350/22L40 (United Kingdom)
BS 2789 400/18 (United Kingdom)
BS 2789 400/18L20 (United Kingdom)
ASME SA395 60-40-18 (USA)
ASTM A356(84) 60-40-18 (USA)
ASTM A395/A395(98) 60-40-18 (USA)
ASTM A536(93) 60-40-18 (USA)
MIL-C-24707/5(89) 60-45-15 (USA)
SAE J434 D4018 (USA)

EN GJS 400 18 Chemical Composition (Cast iron, nodular graphite) | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

Base Fe (Iron) : Fe/3.2-4.1C/1.8-2.8Si/<0.8Mn/<0.1P/<0.03S

EN GJS 400 18 Chemical Composition
EN GJS 400 18 Chemical Composition (Cast iron, nodular graphite)
Material Standards with Similar Chemical Composition
NBN 830-02 FNG38-17 (Belgium)
GB 1348(88) QT 400-15 (China)
GB 1348(88) QT 400-18 (China)
DS 11303 715 (Denmark)
DS 11303 716 (Denmark)
AFNOR NFA32201 FGS350-22 (France)
AFNOR NFA32201 FGS350-22L (France)
AFNOR NFA32201 FGS400-15 (France)
AFNOR NFA32201 FGS400-18 (France)
AFNOR NFA32201 FGS400-18L (France)
DIN WNr 0.7040 (Germany)
DIN WNr 0.7043 (Germany)
DIN 1693 GGG-35.3 (Germany)
DIN 1693 GGG-40 (Germany)
DIN 1693 GGG-40.3 (Germany)
IS 1865 SG370/17 (India)
UNI 4544 GS370-17 (Italy)
JIS G5502(95) FCD37 Class 0 (Japan)
NEN 2733 GN350-22L (Netherlands)
NEN 2733 GN400-15 (Netherlands)
NEN 2733 GN400-18L (Netherlands)
NS 11301 NS11335 (Norway)
NS 11301 NS11338 (Norway)
NS 11301 NS11342 (Norway)
AS 1831(85) 370-17 (NSW Australia)
GOST 7293 VCh35 (Russian Federation)
GOST 7293 VCh40 (Russian Federation)
SABS 936 SG38 (South Africa)
SIS 140717 0717-00 (Sweden)
SIS 140717 0717-02 (Sweden)
SIS 140717 0717-15 (Sweden)
ISO 1083(87) 350-22 (International)
ISO 1083(87) 350-22L (International)
ISO 1083(87) 400-15 (International)
ISO 1083(87) 400-18 (International)
ISO 1083(87) 400-18L (International)
BS 2789 350/22 (United Kingdom)
BS 2789 350/22L40 (United Kingdom)
BS 2789 400/18 (United Kingdom)
BS 2789 400/18L20 (United Kingdom)
ASME SA395 60-40-18 (USA)
ASTM A356(84) 60-40-18 (USA)
ASTM A395/A395(98) 60-40-18 (USA)
ASTM A536(93) 60-40-18 (USA)
MIL-C-24707/5(89) 60-45-15 (USA)
SAE J434 D4018 (USA)

EN GJS 400 15U <30mm Chemical Composition (Cast iron, nodular graphite) | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

Base Fe (Iron) : Fe/3.4-4C/2-2.8Si/<1.0Ni/0.2-0.6Mn/0.02-0.07Mg

EN-GJS-400-15U-lower-than-30mm-Chemical-Composition
EN GJS 400 15U <30mm Chemical Composition (Cast iron, nodular graphite)
Material Standards with Similar Chemical Composition
NBN 830-02 FNG38-17 (Belgium)
GB 1348(88) QT 400-15 (China)
GB 1348(88) QT 400-18 (China)
DS 11303 715 (Denmark)
DS 11303 716 (Denmark)
AFNOR NFA32201 FGS350-22 (France)
AFNOR NFA32201 FGS350-22L (France)
AFNOR NFA32201 FGS400-15 (France)
AFNOR NFA32201 FGS400-18 (France)
AFNOR NFA32201 FGS400-18L (France)
DIN WNr 0.7040 (Germany)
DIN WNr 0.7043 (Germany)
DIN 1693 GGG-35.3 (Germany)
DIN 1693 GGG-40 (Germany)
DIN 1693 GGG-40.3 (Germany)
IS 1865 SG370/17 (India)
UNI 4544 GS370-17 (Italy)
JIS G5502(95) FCD37 Class 0 (Japan)
NEN 2733 GN350-22L (Netherlands)
NEN 2733 GN400-15 (Netherlands)
NEN 2733 GN400-18L (Netherlands)
NS 11301 NS11335 (Norway)
NS 11301 NS11338 (Norway)
NS 11301 NS11342 (Norway)
AS 1831(85) 370-17 (NSW Australia)
GOST 7293 VCh35 (Russian Federation)
GOST 7293 VCh40 (Russian Federation)
SABS 936 SG38 (South Africa)
SIS 140717 0717-00 (Sweden)
SIS 140717 0717-02 (Sweden)
SIS 140717 0717-15 (Sweden)
ISO 1083(87) 350-22 (International)
ISO 1083(87) 350-22L (International)
ISO 1083(87) 400-15 (International)
ISO 1083(87) 400-18 (International)
ISO 1083(87) 400-18L (International)
BS 2789 350/22 (United Kingdom)
BS 2789 350/22L40 (United Kingdom)
BS 2789 400/18 (United Kingdom)
BS 2789 400/18L20 (United Kingdom)
ASME SA395 60-40-18 (USA)
ASTM A356(84) 60-40-18 (USA)
ASTM A395/A395(98) 60-40-18 (USA)
ASTM A536(93) 60-40-18 (USA)
MIL-C-24707/5(89) 60-45-15 (USA)
SAE J434 D4018 (USA)

EN GJS 350 22 LT Chemical Composition (Cast iron, nodular graphite) | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

Base Fe (Iron) : Fe/3.2-4.1C/2-2.5Si/<0.8Mn/<0.04P/<0.03S

EN GJS 350 22 LT Chemical Composition (Cast iron, nodular graphite)
Material Standards with Similar Chemical Composition
NBN 830-02 FNG38-17 (Belgium)
GB 1348(88) QT 400-15 (China)
GB 1348(88) QT 400-18 (China)
DS 11303 715 (Denmark)
DS 11303 716 (Denmark)
AFNOR NFA32201 FGS350-22 (France)
AFNOR NFA32201 FGS350-22L (France)
AFNOR NFA32201 FGS400-15 (France)
AFNOR NFA32201 FGS400-18 (France)
AFNOR NFA32201 FGS400-18L (France)
DIN WNr 0.7040 (Germany)
DIN WNr 0.7043 (Germany)
DIN 1693 GGG-35.3 (Germany)
DIN 1693 GGG-40 (Germany)
DIN 1693 GGG-40.3 (Germany)
IS 1865 SG370/17 (India)
UNI 4544 GS370-17 (Italy)
JIS G5502(95) FCD37 Class 0 (Japan)
NEN 2733 GN350-22L (Netherlands)
NEN 2733 GN400-15 (Netherlands)
NEN 2733 GN400-18L (Netherlands)
NS 11301 NS11335 (Norway)
NS 11301 NS11338 (Norway)
NS 11301 NS11342 (Norway)
AS 1831(85) 370-17 (NSW Australia)
GOST 7293 VCh35 (Russian Federation)
GOST 7293 VCh40 (Russian Federation)
SABS 936 SG38 (South Africa)
SIS 140717 0717-00 (Sweden)
SIS 140717 0717-02 (Sweden)
SIS 140717 0717-15 (Sweden)
ISO 1083(87) 350-22 (International)
ISO 1083(87) 350-22L (International)
ISO 1083(87) 400-15 (International)
ISO 1083(87) 400-18 (International)
ISO 1083(87) 400-18L (International)
BS 2789 350/22 (United Kingdom)
BS 2789 350/22L40 (United Kingdom)
BS 2789 400/18 (United Kingdom)
BS 2789 400/18L20 (United Kingdom)
ASME SA395 60-40-18 (USA)
ASTM A356(84) 60-40-18 (USA)
ASTM A395/A395(98) 60-40-18 (USA)
ASTM A536(93) 60-40-18 (USA)
MIL-C-24707/5(89) 60-45-15 (USA)
SAE J434 D4018 (USA)

EN GJS 350 22 Chemical Composition (Cast iron, nodular graphite) | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

Base Fe (Iron) : Fe/3.2-4.1C/1.8-2.8Si/<0.8Mn/<0.1P/<0.03S

EN GJS 350 22 Chemical Composition (Cast iron, nodular graphite)
Material Standards with Similar Chemical Composition
NBN 830-02 FNG38-17 (Belgium)
GB 1348(88) QT 400-15 (China)
GB 1348(88) QT 400-18 (China)
DS 11303 715 (Denmark)
DS 11303 716 (Denmark)
AFNOR NFA32201 FGS350-22 (France)
AFNOR NFA32201 FGS350-22L (France)
AFNOR NFA32201 FGS400-15 (France)
AFNOR NFA32201 FGS400-18 (France)
AFNOR NFA32201 FGS400-18L (France)
DIN WNr 0.7040 (Germany)
DIN WNr 0.7043 (Germany)
DIN 1693 GGG-35.3 (Germany)
DIN 1693 GGG-40 (Germany)
DIN 1693 GGG-40.3 (Germany)
IS 1865 SG370/17 (India)
UNI 4544 GS370-17 (Italy)
JIS G5502(95) FCD37 Class 0 (Japan)
NEN 2733 GN350-22L (Netherlands)
NEN 2733 GN400-15 (Netherlands)
NEN 2733 GN400-18L (Netherlands)
NS 11301 NS11335 (Norway)
NS 11301 NS11338 (Norway)
NS 11301 NS11342 (Norway)
AS 1831(85) 370-17 (NSW Australia)
GOST 7293 VCh35 (Russian Federation)
GOST 7293 VCh40 (Russian Federation)
SABS 936 SG38 (South Africa)
SIS 140717 0717-00 (Sweden)
SIS 140717 0717-02 (Sweden)
SIS 140717 0717-15 (Sweden)
ISO 1083(87) 350-22 (International)
ISO 1083(87) 350-22L (International)
ISO 1083(87) 400-15 (International)
ISO 1083(87) 400-18 (International)
ISO 1083(87) 400-18L (International)
BS 2789 350/22 (United Kingdom)
BS 2789 350/22L40 (United Kingdom)
BS 2789 400/18 (United Kingdom)
BS 2789 400/18L20 (United Kingdom)
ASME SA395 60-40-18 (USA)
ASTM A356(84) 60-40-18 (USA)
ASTM A395/A395(98) 60-40-18 (USA)
ASTM A536(93) 60-40-18 (USA)
MIL-C-24707/5(89) 60-45-15 (USA)
SAE J434 D4018 (USA)

© Modulus Metal 2017-2022    |    All Rights Reserved