Aluminum A206.0 Mechanical Properties

PropertyMinimumMaximumUnit
Young’s Modulus69.471GPa
Specific Stiffness24.725.5MN.m/kg
Yield Strength (Elastic Limit)333357MPa
Tensile Strength410450MPa
Specific Strength119128kN.m/kg
Elongation7.3914.1% strain
Compressive Strength342389MPa
Flexural Modulus69.471GPa
Flexural Strength (Modulus of Rupture)333357MPa
Shear Modulus26.226.6GPa
Bulk Modulus65.572.4GPa
Poisson’s Ratio0.3230.337–
Shape Factor20––
Hardness (Vickers)130149HV
Elastic Stored Energy (Springs)791908kJ/m³
Fatigue Strength at 10⁷ Cycles195215MPa
Fatigue Strength Model (Stress Range)183229MPa
Aluminum, A206.0, permanent mold cast, T7 | Mechanical PropertiesA12060, A02060 Mechanical PropertiesAMS 4236 Mechanical Properties

MODULUS METAL | ALUMINUM CASTING FOUNDRY IN TURKEY
Aluminium Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, Investment Casting in Turkey, Plaster Casting in Turkey, Heat Treated and CNC Machined Products Manufacturer in Turkey