Aluminum, A206.0, permanent mold cast, T7 Composition

Compositional Summary

Al93-95 / Cu4.2-5 / Mn0.2-0.5 / Mg0.15-0.35 / Ti0.15-0.3 (impurities: Fe<0.1, Zn<0.1, Ni<0.05, Si<0.05, Sn<0.05, Other<0.15)

Composition Details

ElementMinimum (%)Maximum (%)
Al (Aluminum)93.495.3
Cu (Copper)4.25
Fe (Iron)00.1
Mg (Magnesium)0.150.35
Mn (Manganese)0.20.5
Ni (Nickel)00.05
Si (Silicon)00.05
Sn (Tin)00.05
Ti (Titanium)0.150.3
Zn (Zinc)00.1
Other00.15