Standards with Similar Compositions
| Country | Standard/Specification |
|---|---|
| Germany | 3.1371 / AlCu4TiMg to DIN 1725-2 |
| USA | 206, 206.2, A02060 to SAE J452 |
| USA | A201.0 to ASTM B686 |
| USA | A201.0 to MIL A-21180C |
| USA | A206.0, A206.2 |
| USA | UNS A02060, UNS A02062, UNS A12060, UNS A12062 |
| Aluminum, A206.0, permanent mold cast, T7 Equivalent Grades | 3.1371 / AlCu4TiMg to DIN 1725-2 Equivalent Grades |
| Tradenames A206.0 (3.1371 / AlCu4TiMg) |
|---|
| A206 |
Aluminum, A206.0, permanent mold cast, T7 | General information
Aluminum, A206.0, permanent mold cast, T7 | Composition
Aluminum, A206.0, permanent mold cast, T7 | Mechanical Properties
Aluminum, A206.0, permanent mold cast, T7 | Equivalent Grades