Designation
| 6005, wrought | |
| UNS number | A96005 |
| EN name | EN AW-6005 |
Aluminum 6005 Chemical Composition
| Al (aluminum) | 97.5 | – | 99 | % |
| Cr (chromium) | 0 | – | 0.1 | % |
| Cu (copper) | 0 | – | 0.1 | % |
| Fe (iron) | 0 | – | 0.35 | % |
| Mg (magnesium) | 0.4 | – | 0.6 | % |
| Mn (manganese) | 0 | – | 0.1 | % |
| Si (silicon) | 0.6 | – | 0.9 | % |
| Ti (titanium) | 0 | – | 0.1 | % |
| Zn (zinc) | 0 | – | 0.1 | % |
| Other | 0 | – | 0.15 | % |
MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey